Vegard's Law (Alloy Composition)

Get alloy composition x from measured lattice parameter (ideal solution).

CRYSTALLOGRAPHYVerified SI Calculations

Tool Overview & Scientific Scope

Get alloy composition x from measured lattice parameter (ideal solution).

Governing Chemical Equation

a = x·a_A + (1−x)·a_B → x = (a − a_B)/(a_A − a_B)

Input Parameters & Required Units

ParameterAccepted Units / Default
Measured a_alloy (Å) Standard SI
a_A end member (Å) Standard SI
a_B end member (Å) Standard SI

Interactive Calculator & Instant Solver

Runs 100% in your browser using verified physical constants. Edit any value below to recalculate instantly:

← Back to Research Lab Tools