Reduced DP when chain transfer agent is present.
Tool Overview & Scientific Scope
Reduced DP when chain transfer agent is present.
Governing Chemical Equation
1/Xn=1/Xn0+Cs[S]/[M]
Input Parameters & Required Units
| Parameter | Accepted Units / Default |
|---|---|
| Xn0 (no transfer) | Standard SI |
| Transfer constant Cs | Standard SI |
| [S] (mol/L) | Standard SI |
| [M] (mol/L) | Standard SI |