DLS Polydispersity Index

PDI = (σ/d)² from DLS cumulants; PDI<0.1 monodisperse.

NANOCHEMISTRY & NANOMATERIALSVerified SI Calculations

Tool Overview & Scientific Scope

PDI = (σ/d)² from DLS cumulants; PDI<0.1 monodisperse.

Governing Chemical Equation

PDI=(σ/d)²

Input Parameters & Required Units

ParameterAccepted Units / Default
Std dev σ (nm) Standard SI
Mean diameter d (nm) Standard SI

Interactive Calculator & Instant Solver

Runs 100% in your browser using verified physical constants. Edit any value below to recalculate instantly: