Debye Length

Double-layer thickness from ionic strength (water, 298 K).

NANOCHEMISTRY & NANOMATERIALSVerified SI Calculations

Tool Overview & Scientific Scope

Double-layer thickness from ionic strength (water, 298 K).

Governing Chemical Equation

κ⁻¹=√(εkT/(2N_A e²I))

Input Parameters & Required Units

ParameterAccepted Units / Default
ε_r Standard SI
T (K) Standard SI
I (mol/L) Standard SI

Interactive Calculator & Instant Solver

Runs 100% in your browser using verified physical constants. Edit any value below to recalculate instantly: