Lattice Energy and Born-Haber Cycles
Born-Lande equation, Kapustinskii, and thermochemical cycles.
Assessment Overview: 5 multiple-choice questions assessing conceptual and mathematical proficiency in Lattice Energy and Born-Haber Cycles.
Practice Questions & Answers
Question 1: Lattice energy is defined as the energy:
- A. To form the solid
- B. To separate 1 mol of solid into gaseous ions (Correct Answer)
- C. To melt the solid
- D. To ionize atoms
Pedagogical Explanation: M⁺(g) + X⁻(g) → MX(s): ΔH_lattice.
Question 2: Lattice formation from gaseous ions is:
- A. Endothermic
- B. Zero
- C. Exothermic (Correct Answer)
- D. Impossible
Pedagogical Explanation: Ion combination releases energy.
Question 3: The Born-Lande equation includes:
- A. Temperature
- B. Madelung constant, charges, distance, Born exponent (Correct Answer)
- C. Only charges
- D. Only distance
Pedagogical Explanation: U = −N_A M z⁺z⁻e²/(4πε₀r₀)(1−1/n).
Question 4: The Madelung constant accounts for:
- A. Repulsion
- B. Temperature
- C. Pressure
- D. Geometry of all ion interactions (Correct Answer)
Pedagogical Explanation: Sums Coulomb attractions/repulsions over the lattice.
Question 5: The Born exponent n accounts for:
- A. Attraction
- B. Short-range repulsion (Correct Answer)
- C. Magnetism
- D. Temperature
Pedagogical Explanation: Repulsion from overlapping electron clouds.