Fertilizer, water-quality and industrial numerics dominate; sulfur-cycle questions are a small strand.

ENVIRONMENTAL5 QuestionsPractice Quiz
Assessment Overview: 5 multiple-choice questions assessing conceptual and mathematical proficiency in Fertilizers, Water & Industrial Numerics Practice.

Practice Questions & Answers

Question 1: Winkler titration: 9.5 mL of 0.05 N Na₂S₂O₃ used for a 200 mL sample. Dissolved oxygen?

  • A. 20 mg/L
  • B. 19 mg/L (Correct Answer)
  • C. 38 mg/L
  • D. 9.5 mg/L
Pedagogical Explanation: DO = V(thio) × N × 8000 / V(sample) = 9.5 × 0.05 × 8000/200 = 19 mg/L.

Question 2: In the Haber reactor, 5 mol N₂ and 15 mol H₂ react with 30% conversion of N₂. Moles of NH₃ at equilibrium?

  • A. 4.5 mol
  • B. 3 mol (Correct Answer)
  • C. 3.5 mol
  • D. 1.5 mol
Pedagogical Explanation: NH₃ formed = 2 × (mol N₂ reacted) = 2 × 5 × 30/100 = 3 mol.

Question 3: How much nitrogen is contained in 410 kg of urea, CO(NH₂)₂?

  • A. 205 kg N
  • B. 218.5 kg N
  • C. 191.5 kg N (Correct Answer)
  • D. 248.9 kg N
Pedagogical Explanation: urea, CO(NH₂)₂ is 46.7% N (M = 60, N mass = 28 → 46.7%), so 410 × 46.7/100 = 191.5 kg N.

Question 4: A city generates 1293 t of municipal waste per day and recycles 491 t. Recycling rate?

  • A. 38 % (Correct Answer)
  • B. 48 %
  • C. 379.7 %
  • D. 19 %
Pedagogical Explanation: Recycling rate = recycled/generated × 100 = 491/1293 × 100 = 38%.

Question 5: Limestone calcination: how much CaO from 727 t of CaCO₃?

  • A. 325.7 tonnes
  • B. 203.6 tonnes
  • C. 814.2 tonnes
  • D. 407.1 tonnes (Correct Answer)
Pedagogical Explanation: CaCO₃ (100) → CaO (56): 727 × 0.56 = 407.1 t.