CHEMVEN

SNOM (Near-Field Scanning Optical Microscope)

Optical imaging beyond diffraction via near field

MICROSCOPYAnalytical Instrument

Operational Principle

Scanning near-field optical microscopy beats the diffraction limit by collecting or delivering light through a sub-wavelength aperture (or sharp tip) held nanometers from the surface.

Optical & Mechanical Architecture

In aperture SNOM, laser light exits a metal-coated tapered fiber with a ~50–100 nm aperture; because the aperture sits within the near field (<λ) of the sample, resolution is set by aperture size (~50–100 nm), not wavelength. Apertureless (scattering) SNOM instead focuses light onto a sharp AFM tip that scatters the near field, reaching ~10–20 nm; demodulating the signal at the tip's tapping frequency isolates the near-field component from far-field background. Both combine optical spectroscopy with AFM topography.

Applications in Research & Industry

Nanoscale optical mapping of photonic crystals and waveguides,Plasmonic hot-spot and nanoantenna field imaging,Single-molecule fluorescence near-field studies,Semiconductor defect luminescence at ~50 nm

Typical Performance Specifications

Resolution ~50–100 nm (aperture) · ~10–20 nm (scattering tip) · combined AFM topography · fiber or cantilever probes

Operational Visualization Notes

microscope

← Back to Instruments Hub