CHEMVEN

Pressure DSC

Calorimetry under gas pressure

THERMAL ANALYSISAnalytical Instrument

Operational Principle

Runs DSC inside a pressurized chamber — essential when oxidation, curing, or volatile loss would escape or behave differently at ambient pressure.

Optical & Mechanical Architecture

The sealed cell holds up to ~70 bar of gas (O₂, N₂, H₂) while temperature ramps. Pressurized oxygen accelerates oxidative stability tests (OIT of polymers); pressure suppresses solvent evaporation so curing and crystallization are measured cleanly.

Applications in Research & Industry

Polymer oxidative induction time,Resin cure under pressure,Volatile-containing samples,Hydrogenation reaction heats

Typical Performance Specifications

Up to ~70 bar · O₂/N₂/H₂ atmospheres · −100 to 700 °C

Operational Visualization Notes

thermal