Magnetic Force Microscope (MFM)

Nanoscale magnetic domain imaging with a tip

MICROSCOPYAnalytical Instrument

Operational Principle

The magnetic force microscope maps magnetic domains and stray fields at ~50 nm resolution using a magnetized AFM tip scanned in lift mode above the surface.

Optical & Mechanical Architecture

A cantilever coated with a ferromagnetic film (CoCr, ~30–50 nm) is first scanned in tapping mode to record topography; it then retraces the same line lifted 20–100 nm above the surface, where only long-range magnetic forces act. The tip–sample magnetic interaction shifts the cantilever's resonant frequency or phase, producing a map of the stray-field gradient — domain walls and bits appear as contrast. Two-pass lift mode cleanly separates magnetic from topographic signals.

Applications in Research & Industry

Hard-disk bit and domain-wall imaging,Magnetic nanoparticle and thin-film domain studies,Spintronic device and MRAM characterization,Superconducting vortex lattice imaging

Typical Performance Specifications

Lateral resolution ~30–50 nm · lift height 20–100 nm · CoCr-coated tips · phase/frequency-shift detection · two-pass mode

Operational Visualization Notes