Limiting Oxygen Index Tester
How much oxygen a plastic needs to burn
Operational Principle
Finds the minimum oxygen concentration that keeps a material burning — the single number (LOI %) behind most polymer flammability ratings.
Optical & Mechanical Architecture
A vertical sample burns in a glass chimney fed with a controlled O₂/N₂ mix. The O₂ fraction is adjusted until the sample just sustains flame for 3 minutes or 50 mm. LOI above ~27% means self-extinguishing in air; below 21% burns freely.
Applications in Research & Industry
Plastic flame-retardant grading,Textile flammability,Cable insulation specs,Foam safety testing
Typical Performance Specifications
O₂/N₂ mixing column · LOI % readout · ASTM D2863