Heat Deflection Temperature Tester
Load-bearing heat resistance of plastics
Operational Principle
Measures the temperature at which a plastic bar deflects 0.25 mm under a standard bending load — how hot a part can get before it sags in service.
Optical & Mechanical Architecture
A bar specimen is loaded in three-point bending (0.45 or 1.8 MPa fiber stress) in a heated oil bath ramping at 2 °C/min. The deflection-vs-temperature curve gives the HDT — the design limit for under-hood, electrical, and structural plastic parts.
Applications in Research & Industry
Engineering plastic selection,Under-hood part design,Electrical housing specs,Composite benchmarking
Typical Performance Specifications
0.45 / 1.8 MPa stress · 2 °C/min · 0.25 mm deflection criterion
Operational Visualization Notes
thermal