CHEMVEN

Glow Discharge Optical Emission Spectrometer (GD-OES)

Depth-profiles coatings, layer by atomic layer

SPECTROSCOPYAnalytical Instrument

Operational Principle

Sputters a solid sample with a low-pressure argon plasma and reads the emission of eroded atoms, producing quantitative concentration-vs-depth profiles of coatings, galvanized steel, nitrided layers and thin films.

Optical & Mechanical Architecture

The sample acts as the cathode in a Grimm-type glow discharge (Ar, ~500–1000 Pa, DC or RF at 13.56 MHz); Ar⁺ ions sputter atoms uniformly from a 4 mm crater at 10–100 nm/s while a polychromator records emission lines in real time. Because sputtering is stoichiometric for metals, intensity-vs-time converts directly to concentration-vs-depth with ~5 nm interface resolution — faster and cheaper than SIMS for micrometer-thick coatings.

Applications in Research & Industry

Galvanized and painted steel coating analysis,Hardened-case depth in nitrided gears,Solar-cell and display multilayer stacks,Hydrogen and light-element profiling in metals

Typical Performance Specifications

Depth resolution ~5 nm · sputter rate 10–100 nm/s · detects H–U incl. H, C, N, O · crater Ø 4 mm · RF for insulators

Operational Visualization Notes

plasma

← Back to Instruments Hub