Electrogravimetry Cell
Weighing metals deposited by electrolysis
Operational Principle
Determines metal concentration by plating it quantitatively onto an electrode and weighing the deposit — one of the oldest and most accurate absolute methods.
Optical & Mechanical Architecture
A weighed platinum gauze electrode is held at a potential that reduces only the target metal ion; after complete deposition it is rinsed, dried, and reweighed. The mass gain equals metal plated. Still the reference method for copper and nickel assays.
Applications in Research & Industry
Copper/nickel assay,Plating-bath control,Precious-metal recovery checks,Teaching quantitative analysis
Typical Performance Specifications
Pt gauze electrode · 0.1 mg balance sensitivity · ±0.1% accuracy