Dynamic Mechanical Analyzer (DMA)
Viscoelastic fingerprint of polymers vs temperature
Operational Principle
An instrument that applies a small oscillatory force to a sample while ramping temperature, measuring storage modulus (E′), loss modulus (E″), and tan δ to locate glass transitions and map viscoelastic behavior.
Optical & Mechanical Architecture
The sample (film, bar, or fiber in tension, bending, or shear fixtures) is deformed sinusoidally (typically 1 Hz) as temperature ramps. The in-phase response gives stiffness E′, the out-of-phase response gives damping E″, and the tan δ peak marks the glass transition Tg.
Applications in Research & Industry
Glass-transition and secondary-relaxation mapping of polymers,Cure monitoring and crosslink-density estimation,Damping performance of composites and adhesives
Typical Performance Specifications
Temp −150 to 600 °C; frequency 0.01–200 Hz; modulus 10³–3×10¹² Pa; strain 0.1 µm–10 mm; heating 0.1–20 °C/min
Operational Visualization Notes
thermal