CHEMVEN

DSC Principle: Heat Capacity Step at the Glass Transition (Data Study)

To interpret a DSC trace: glass transition, crystallisation exotherm and melting endotherm.

Level: UniversitySafety: SafeTime: 45 min
Aim of Experiment: To interpret a DSC trace: glass transition, crystallisation exotherm and melting endotherm.

Theoretical Foundations

Differential scanning calorimetry measures heat flow vs a reference on heating. A glass transition appears as a step in baseline (ΔCp, no latent heat); cold crystallisation as an exotherm; melting as an endotherm whose area = ΔH_fus. Reading a PET trace (Tg ≈ 75 °C, Tm ≈ 250 °C) teaches modern thermal analysis without the instrument.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Printed DSC traces (PET sample and indium standard)
  • Calculator
  • Ruler
  • Notebook
  • Data booklet (thermal analysis reference values)

Chemical Reagents

    Step-by-Step Practical Procedure

    1. Study the PET DSC trace: identify the Tg step, crystallisation exotherm, melting endotherm.
    2. Measure the melting peak area; convert to ΔH_fus using the indium calibration.
    3. Read Tg from the midpoint of the Cp step.
    4. Explain why Tg shows no peak (second-order-like transition).
    5. Discuss what crystallinity % = ΔH_obs/ΔH_100% gives.

    Observations & Expected Results

    Data study: PET shows Tg step at ~75 °C, crystallisation exotherm ~130 °C, melting endotherm ~250 °C with ΔH ≈ 40 J/g → ~29% crystalline (vs 140 J/g fully crystalline).

    Worked Stoichiometric Calculations

    Problem: A PET sample's melting endotherm area corresponds to 40 J/g; 100% crystalline PET ΔH_fus = 140 J/g. Find the crystallinity.

    Working: Crystallinity = 40/140 × 100% = 28.6% — typical for commercial PET film; the rest is amorphous (hence the visible Tg step).

    Safety Precautions & Hazard Control

    • No chemicals; classroom safety only.
    • Keep track of units (J vs kJ) throughout the calculation.
    • Watch sign conventions: exothermic changes are negative.
    • Use kelvin for any temperature inside a logarithm or 1/T term.

    Waste Disposal Protocol

    No waste.

    Viva Voce Oral Defense Questions & Answers

    Q: What does DSC actually measure?

    A: The differential heat flow needed to keep sample and reference at the same temperature during a controlled heating programme.

    Q: Why is the glass transition a step, not a peak?

    A: No latent heat is involved — only the heat capacity changes as frozen molecular motions unlock.

    Q: How is the instrument calibrated?

    A: With high-purity indium (Tm = 156.6 °C, ΔH_fus = 28.6 J/g) — a sharp, certified melting endotherm.

    ← Back to Experiments Directory