CHEMVEN

Adsorption of a Gas on a Solid: CO2 on Charcoal by Weight Gain

To measure gas adsorption directly by weighing charcoal before and after exposure to CO2.

Level: UniversitySafety: SafeTime: 60 min
Aim of Experiment: To measure gas adsorption directly by weighing charcoal before and after exposure to CO2.

Theoretical Foundations

Charcoal's huge surface area adsorbs gases physically (van der Waals). Passing CO2 over dry, pre-weighed charcoal increases its mass; the uptake per gram at 1 atm characterises the adsorbent - the principle of gas masks and storage.

Required Apparatus & Chemicals

Laboratory Apparatus

  • U-tube or gas-adsorption tube
  • Analytical balance
  • CO2 source (Kipp's or cylinder)
  • Drying tube (CaCl2)

Chemical Reagents

  • Activated charcoal (dried)
  • Carbon dioxide gas
  • Calcium chloride (drying)

Step-by-Step Practical Procedure

  1. Dry charcoal at 110 C; weigh the adsorption tube filled with it.
  2. Pass dry CO2 slowly through for 20 min.
  3. Reweigh; find mass gain.
  4. Calculate uptake (mg CO2 per g charcoal).
  5. Warm the tube gently - note desorption (mass falls).

Observations & Expected Results

Typical student data: 5.00 g charcoal gains ~0.35 g CO2 (~70 mg/g); warming drives most of it off - reversible physical adsorption.

Worked Stoichiometric Calculations

Problem: 5.00 g charcoal gains 0.35 g CO2 (M = 44.0). What is the uptake in mmol/g?

Working: Moles = 0.35/44.0 = 7.95 x 10^-3 mol. Uptake = 7.95/5.00 = 1.59 mmol/g.

Safety Precautions & Hazard Control

  • Dry the charcoal and the gas - water competes for sites.
  • Weigh quickly (CO2 desorbs in air).
  • Keep gas flow slow for equilibration.

Waste Disposal Protocol

Charcoal reusable after heating; no hazardous waste.

Viva Voce Oral Defense Questions & Answers

Q: Why must the charcoal be dried first?

A: Adsorbed water blocks pores and would be displaced confusingly by CO2.

Q: Why does warming reverse adsorption?

A: Physical adsorption is exothermic; heating shifts equilibrium toward desorption.

Q: Name two applications.

A: Gas masks (toxic vapour adsorption) and CO2 capture/storage research.

← Back to Experiments Directory