Catalyst and Equilibrium: MnO2 Does Not Shift the H2O2 Equilibrium Position

Prove that a catalyst changes the rate but not the position of equilibrium, using H2O2 decomposition with and without MnO2.

Level: UniversitySafety: Needs supervisionTime: 60 min
Aim of Experiment: Prove that a catalyst changes the rate but not the position of equilibrium, using H2O2 decomposition with and without MnO2.

Theoretical Foundations

A catalyst lowers Ea for forward and reverse reactions equally, so k_forward and k_reverse increase by the same factor and K = k_f/k_r is unchanged. The final O2 volume (extent of reaction) should be identical with and without MnO2; only the time to reach it differs.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Two side-arm flasks
  • Gas syringes
  • Stopwatches
  • Balance
  • Water bath at 25 C

Chemical Reagents

  • Hydrogen peroxide, 20-volume
  • Manganese(IV) oxide powder
  • Distilled water

Step-by-Step Practical Procedure

  1. Set up two identical assemblies with 25 mL H2O2 at 25 C.
  2. Add 0.5 g MnO2 to one; leave the other uncatalysed.
  3. Record O2 volumes until both stop changing (the uncatalysed run takes much longer; use a smaller H2O2 volume or KI catalyst to speed it).
  4. Compare the final volumes Vinf.
  5. Compare the times to reach Vinf.

Observations & Expected Results

Typical student data: both flasks reach Vinf ~ 290 mL; the catalysed run finishes in ~30 min while the uncatalysed takes many hours: same extent, different rate.

Worked Stoichiometric Calculations

Problem: Typical student data: Vinf = 290 mL in both flasks; t(complete) = 30 min (catalysed) vs 1200 min (uncatalysed). What is shown?

Working: Identical Vinf proves the equilibrium position (extent) is unchanged; the 40-fold faster completion proves the catalyst changes only the rate.

Safety Precautions & Hazard Control

  • The uncatalysed run is very slow; plan timing or use mild warming consistently for both.
  • Ensure both assemblies are gas-tight.
  • H2O2 irritates skin.

Waste Disposal Protocol

Filter and reuse MnO2; dilute filtrate to the sink.

Viva Voce Oral Defense Questions & Answers

Q: Why is K unchanged?

A: K = k_f/k_r; the catalyst lowers both barriers equally, so both rate constants scale by the same factor.

Q: Draw the energy profiles.

A: Same reactants and products energy levels; the catalysed path has a lower hump but identical endpoints.

Q: Can a catalyst ever change the yield?

A: Only the rate of reaching it; the equilibrium yield is fixed by thermodynamics.