CHEMVEN

Depolariser Action of Manganese Dioxide

To show that MnO2 prevents polarisation in the simple voltaic cell.

Level: UniversitySafety: Needs supervisionTime: 45 min
Aim of Experiment: To show that MnO2 prevents polarisation in the simple voltaic cell.

Theoretical Foundations

MnO2 oxidises the polarising hydrogen: 2MnO2 + H2 -> Mn2O3 + H2O. Packed around the carbon cathode (as in the Leclanche cell), it continuously removes H2, keeping the EMF steady - the definition of a depolariser.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Zn rod
  • Carbon rod
  • Beaker
  • Voltmeter
  • Bulb
  • Muslin bag

Chemical Reagents

  • Ammonium chloride solution (1 M)
  • Manganese dioxide powder
  • Distilled water (for rinsing glassware and electrodes)

Step-by-Step Practical Procedure

  1. Set up Zn|NH4Cl|C and record how fast the EMF falls under load.
  2. Pack MnO2 around the carbon rod in a muslin bag.
  3. Re-measure the EMF decay under the same load.
  4. Compare the two decay curves.
  5. Conclude on the depolariser's effect.

Observations & Expected Results

Without MnO2 the voltage sags within minutes; with MnO2 it stays near 1.4 V much longer.

Worked Stoichiometric Calculations

Problem: Write the depolariser reaction and identify the oxidant and reductant.

Working: 2MnO2 + H2 -> Mn2O3 + H2O. MnO2 is the oxidant (Mn(IV) -> Mn(III)); H2 is the reductant (0 -> +1).

Safety Precautions & Hazard Control

  • Avoid MnO2 dust inhalation.
  • NH4Cl solution is a mild irritant.
  • Switch off the power supply before changing any connections.

Waste Disposal Protocol

MnO2 sludge to solid chemical waste.

Viva Voce Oral Defense Questions & Answers

Q: What is a depolariser?

A: A substance that removes the polarising product (here H2) from the electrode, keeping the cell voltage steady.

Q: Where is this used commercially?

A: In Leclanche dry cells and zinc-carbon batteries, where MnO2 surrounds the carbon cathode.