CHEMVEN

Hydrogen Overvoltage on Different Cathode Metals

To compare the hydrogen evolution overvoltage on Pt, Cu and Pb cathodes.

Level: UniversitySafety: Needs supervisionTime: 60 min
Aim of Experiment: To compare the hydrogen evolution overvoltage on Pt, Cu and Pb cathodes.

Theoretical Foundations

The reversible H+/H2 potential is 0.00 V, but extra voltage (overvoltage eta) is needed to evolve H2 at a practical rate. eta is tiny on Pt (~0.07 V) and huge on Pb (~0.8 V) because H adsorption energetics differ. High overvoltage on Pb is why lead-acid batteries can be charged without gassing excessively.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Pt, Cu and Pb wire cathodes
  • Graphite anode
  • Beaker
  • DC supply
  • Voltmeter
  • Reference electrode (calomel)

Chemical Reagents

  • Sulphuric acid (0.5 M)
  • Distilled water (for rinsing)
  • Sodium bicarbonate (for neutralising acid spills)

Step-by-Step Practical Procedure

  1. Set up the cell with the Pt cathode and calomel reference.
  2. Raise the voltage until steady H2 bubbles appear; record the cathode potential.
  3. Repeat with Cu and Pb cathodes at the same current.
  4. Compute eta = E(cathode) - 0.00 V for each.
  5. Rank the metals by overvoltage.

Observations & Expected Results

Typical eta: Pt ~0.1 V, Cu ~0.4 V, Pb ~0.8 V at the same current density.

Worked Stoichiometric Calculations

Problem: The Pb cathode sits at -0.80 V vs SHE while evolving H2 at 10 mA/cm2. What is the hydrogen overvoltage?

Working: eta = |-0.80 - 0.00| = 0.80 V.

Safety Precautions & Hazard Control

  • Lead is toxic; wear gloves and avoid ingestion.
  • Vent H2 safely.
  • Switch off the power supply before changing any connections.

Waste Disposal Protocol

Lead waste to the lead-waste container; acid neutralised before disposal.

Viva Voce Oral Defense Questions & Answers

Q: Define overvoltage.

A: The excess potential beyond the reversible (thermodynamic) value required to drive an electrode reaction at a given rate.

Q: Why is high hydrogen overvoltage on lead useful?

A: It lets the lead-acid cell charge at ~2.4 V without wasting all the current on H2 evolution.

← Back to Experiments Directory