Identifying Anode and Cathode from Cell Polarity

To identify the anode and cathode of unknown metal pairs from voltmeter polarity.

Level: UniversitySafety: SafeTime: 40 min
Aim of Experiment: To identify the anode and cathode of unknown metal pairs from voltmeter polarity.

Theoretical Foundations

In a galvanic cell the anode is the negative terminal (site of oxidation) and the cathode is the positive terminal (site of reduction). The metal with the more negative standard electrode potential becomes the anode. Measuring polarity therefore reveals the relative order of metals in the electrochemical series.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Strips of Zn, Fe, Cu, Mg
  • 100 mL beakers
  • Salt bridges
  • Digital voltmeter
  • Connecting wires
  • Sandpaper

Chemical Reagents

  • ZnSO4 (1.0 M)
  • FeSO4 (1.0 M)
  • CuSO4 (1.0 M)
  • MgSO4 (1.0 M)

Step-by-Step Practical Procedure

  1. Build a Zn-Fe cell and note which electrode connects to the positive voltmeter lead.
  2. Repeat for the Fe-Cu, Zn-Cu and Mg-Zn pairs.
  3. Tabulate the negative (anode) metal for each pair.
  4. Arrange the four metals in order of increasing tendency to oxidise.
  5. Compare your order with the standard electrochemical series.

Observations & Expected Results

Zn is negative vs Cu and Fe but positive vs Mg. Order obtained: Mg > Zn > Fe > Cu (most easily oxidised first), matching the series.

Worked Stoichiometric Calculations

Problem: Edeg(Mg2+/Mg) = -2.37 V and Edeg(Fe2+/Fe) = -0.44 V. For an Mg-Fe cell, which metal is the anode and what is Edegcell?

Working: Mg has the more negative potential, so Mg is oxidised: Mg is the anode (negative terminal). Edegcell = -0.44 - (-2.37) = 1.93 V.

Safety Precautions & Hazard Control

  • Clean Mg ribbon surface; its oxide layer gives erratic readings.
  • Keep FeSO4 solutions fresh; they oxidise in air.
  • Switch off the power supply before changing any connections.

Waste Disposal Protocol

Collect metal salt solutions in the heavy-metal waste container.

Viva Voce Oral Defense Questions & Answers

Q: In a galvanic cell, is the anode positive or negative?

A: Negative - oxidation releases electrons, leaving the anode electron-rich relative to the cathode.

Q: Does this sign convention hold for electrolytic cells?

A: No. In an electrolytic cell the anode is positive because an external supply drives oxidation there.