CHEMVEN

Effect of Electrode Size on EMF and Current Output

To show that cell EMF is independent of electrode size while current capacity depends on it.

Level: UniversitySafety: SafeTime: 45 min
Aim of Experiment: To show that cell EMF is independent of electrode size while current capacity depends on it.

Theoretical Foundations

EMF is an intensive property: it depends on the nature of the electrode reactions and ion activities, not on the amount of material. Larger electrodes have lower internal resistance and larger surface area, so they can deliver more current, but the open-circuit voltage is unchanged.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Large and small Zn strips
  • Large and small Cu strips
  • Two 100 mL beakers
  • Salt bridge
  • Digital voltmeter
  • Low-voltage bulb or ammeter
  • Connecting wires

Chemical Reagents

  • ZnSO4 (1.0 M)
  • CuSO4 (1.0 M)
  • KNO3 (salt bridge)

Step-by-Step Practical Procedure

  1. Build a Daniell cell with the large electrodes and record the open-circuit EMF.
  2. Rebuild with the small electrodes in fresh solutions and record the EMF.
  3. Connect the bulb across the large-electrode cell and note its brightness.
  4. Connect the bulb across the small-electrode cell and compare brightness.
  5. Measure the short-circuit current with the ammeter for both cells.

Observations & Expected Results

Both cells read ~1.10 V open-circuit. The large-electrode cell lights the bulb more brightly and gives a higher short-circuit current.

Worked Stoichiometric Calculations

Problem: A Daniell cell has EMF 1.10 V and internal resistance 3 ohm. What current flows through a 7 ohm external load, and what is the terminal voltage?

Working: Total resistance = 3 + 7 = 10 ohm. Current I = 1.10/10 = 0.11 A. Terminal voltage V = E - Ir = 1.10 - 0.11 x 3 = 1.10 - 0.33 = 0.77 V.

Safety Precautions & Hazard Control

  • Do not short the cell for long; it depletes the electrodes.
  • Use the correct ammeter range to avoid blowing the fuse.
  • Switch off the power supply before changing any connections.

Waste Disposal Protocol

Return electrolyte solutions to the heavy-metal waste bottle.

Viva Voce Oral Defense Questions & Answers

Q: Why does EMF not change with electrode size?

A: EMF depends on the electrode potential, which is fixed by the redox couple and ion activities - both intensive quantities.

Q: Why does the bigger cell give more current?

A: Larger surface area means lower internal resistance and more reaction sites, so more charge per second can be transferred.

← Back to Experiments Directory