CHEMVEN

Adsorption Capacity: How Much Charcoal is Enough?

Measure charcoal's adsorption isotherm crudely: decolourise dye solutions with increasing charcoal doses.

Level: UniversitySafety: SafeTime: 50 min
Aim of Experiment: Measure charcoal's adsorption isotherm crudely: decolourise dye solutions with increasing charcoal doses.

Theoretical Foundations

Adsorption follows isotherm behaviour (Freundlich/Langmuir): uptake rises with dose but with diminishing returns as sites fill. Adding 0.1–2.0 g charcoal to fixed dye volumes and measuring residual colour (colorimeter or visual scale) plots the isotherm — the quantitative basis for 'use the minimum effective charcoal' in recrystallisations.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Conical flasks
  • Filter funnels
  • Colorimeter or phone app
  • Balance

Chemical Reagents

  • Methylene blue solution (0.01%, 6 x 50 mL)
  • Activated charcoal (0.1-2.0 g portions)
  • Distilled water (for rinsing)

Step-by-Step Practical Procedure

  1. Add graded charcoal masses to the six dye solutions; shake 10 min.
  2. Filter; measure residual absorbance.
  3. Plot absorbance vs charcoal mass.
  4. Find the dose giving ~95% decolourisation; note the wastefulness beyond it.

Observations & Expected Results

Absorbance falls steeply then plateaus: e.g. 0.5 g removes 95%, 2.0 g removes 98% — four times the charcoal for 3% more colour.

Worked Stoichiometric Calculations

Problem: 0.5 g charcoal removed 95% of 5 mg dye (50 mL of 0.01%). Calculate the loading in mg dye per g charcoal, and the cost of chasing 99%.

Working: Adsorbed = 4.75 mg → loading = 9.5 mg/g. Chasing 99% needed ~1.5 g for 4.95 mg → marginal loading collapses: the last 4% of colour costs 3× the charcoal — and adsorbs product too. Stop at the knee of the curve.

Safety Precautions & Hazard Control

  • Methylene blue stains — gloves, lab coat.
  • Filter charcoal fully; fines in the filtrate fake the reading.
  • Don't ingest.

Waste Disposal Protocol

Charcoal to solid waste; filtrates to aqueous waste.

Viva Voce Oral Defense Questions & Answers

Q: Why does the curve plateau?

A: Finite surface sites: once covered, extra charcoal adds little — the Langmuir saturation behind the rule of minimum effective dose.

Q: How does this change recrystallisation practice?

A: Use charcoal sparingly and briefly: excess adsorbs your product as well as the colour, costing yield for no purity gain.

← Back to Experiments Directory