CHEMVEN

Turnbull's Blue from Ferrous Sulfate

To prepare Turnbull's blue by reacting ferrous sulfate with potassium ferricyanide.

Level: UniversitySafety: Needs supervisionTime: 45 min
Aim of Experiment: To prepare Turnbull's blue by reacting ferrous sulfate with potassium ferricyanide.

Theoretical Foundations

Ferrous ions with ferricyanide give a deep blue precipitate: 3FeSO4 + 2K3[Fe(CN)6] → Fe3[Fe(CN)6]2↓ + 3K2SO4. X-ray studies show Turnbull's blue is identical to Prussian blue (electron transfer makes Fe(III)–Fe(II) equivalent).

Required Apparatus & Chemicals

Laboratory Apparatus

  • 500 mL beaker
  • Glass rod
  • Funnel
  • Filter paper
  • Weighing balance
  • Oven

Chemical Reagents

  • Ferrous sulfate heptahydrate, FeSO4·7H2O (8.34 g)
  • Potassium ferricyanide, K3[Fe(CN)6] (6.58 g)
  • Distilled water (250 mL)
  • Dilute H2SO4 (few drops)

Step-by-Step Practical Procedure

  1. Dissolve 8.34 g FeSO4·7H2O in 100 mL water acidified with a few drops of dilute H2SO4.
  2. Dissolve 6.58 g K3[Fe(CN)6] in 100 mL water.
  3. Add the ferricyanide solution to the ferrous solution with stirring.
  4. A deep blue precipitate forms immediately.
  5. Filter, wash with hot water until washings are colourless.
  6. Dry at 100 °C, grind, and weigh.

Observations & Expected Results

Dark blue powder indistinguishable from Prussian blue; typical yield 5.2–5.7 g.

Worked Stoichiometric Calculations

Problem: 8.34 g FeSO4·7H2O (M = 278.01) reacts with excess ferricyanide. Calculate the theoretical yield of Fe3[Fe(CN)6]2 (M = 591.37). If 5.4 g is obtained, find the percentage yield.

Working: Moles FeSO4·7H2O = 8.34/278.01 = 0.0300 mol. Three moles give one mole of product = 0.0100 mol. Theoretical mass = 0.0100 × 591.37 = 5.91 g. Percentage yield = (5.4/5.91) × 100 = 91.4%.

Safety Precautions & Hazard Control

  • Keep the ferrous solution slightly acidic to prevent oxidation.
  • Work quickly; Fe(II) oxidizes in air.
  • Do not heat with concentrated acids.
  • Wash the precipitate thoroughly.

Waste Disposal Protocol

Cyanide-complex residues are treated with alkaline hypochlorite before disposal.

Viva Voce Oral Defense Questions & Answers

Q: How does Turnbull's blue relate to Prussian blue?

A: They are the same compound; rapid electron transfer makes them identical.

Q: Write the formation equation.

A: 3FeSO4 + 2K3[Fe(CN)6] → Fe3[Fe(CN)6]2 + 3K2SO4.

Q: Why is the ferrous solution kept acidic?

A: To prevent aerial oxidation of Fe(II) to Fe(III).

← Back to Experiments Directory