CHEMVEN

Schönite (Picromerite): A Double Sulfate Salt

To prepare the double salt schönite, K2SO4·MgSO4·6H2O, by crystallization.

Level: UniversitySafety: SafeTime: 60 min
Aim of Experiment: To prepare the double salt schönite, K2SO4·MgSO4·6H2O, by crystallization.

Theoretical Foundations

Unlike Mohr's salt, schönite is a double salt of two sulfates with different cations: K2SO4 + MgSO4 + 6H2O → K2SO4·MgSO4·6H2O. It crystallizes from equimolar mixed solutions and is a source of potassium in fertilizers.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 250 mL beaker
  • Glass rod
  • Weighing balance
  • Bunsen burner
  • China dish
  • Funnel
  • Filter paper

Chemical Reagents

  • Potassium sulfate, K2SO4 (17.43 g)
  • Magnesium sulfate heptahydrate, MgSO4·7H2O (24.65 g)
  • Distilled water (100 mL)

Step-by-Step Practical Procedure

  1. Dissolve 17.43 g K2SO4 in 60 mL warm water.
  2. Dissolve 24.65 g MgSO4·7H2O in 40 mL warm water.
  3. Mix the two clear solutions in a china dish.
  4. Evaporate gently to the crystallization point.
  5. Cool slowly; colourless crystals of schönite separate.
  6. Filter, wash with a little cold water, dry between filter papers, and weigh.

Observations & Expected Results

Colourless monoclinic crystals; typical yield 34–38 g.

Worked Stoichiometric Calculations

Problem: 17.43 g K2SO4 (M = 174.26) and 24.65 g MgSO4·7H2O (M = 246.47) are mixed. Calculate the theoretical yield of schönite K2SO4·MgSO4·6H2O (M = 402.72). If 35.0 g is obtained, find the percentage yield.

Working: Moles K2SO4 = 17.43/174.26 = 0.100 mol; moles MgSO4·7H2O = 24.65/246.47 = 0.100 mol → 0.100 mol schönite. Theoretical mass = 0.100 × 402.72 = 40.3 g. Percentage yield = (35.0/40.3) × 100 = 86.9%.

Safety Precautions & Hazard Control

  • Dissolve each salt fully before mixing.
  • Evaporate gently; do not boil dry.
  • Cool slowly for well-formed crystals.
  • Store in a stoppered bottle; the salt effloresces slightly.

Waste Disposal Protocol

Mother liquor contains potassium and magnesium sulfates; dispose via inorganic aqueous waste.

Viva Voce Oral Defense Questions & Answers

Q: What is a double salt?

A: A crystalline compound of two salts that dissociates into its ions in solution, e.g., K2SO4·MgSO4·6H2O.

Q: How does a double salt differ from a complex salt?

A: A double salt gives all its constituent ions in solution; a complex salt gives complex ions.

Q: Name a fertilizer use of schönite.

A: It supplies both potassium and magnesium to soils.

← Back to Experiments Directory