CHEMVEN

Cobalt Hydroxide by Precipitation (Blue to Pink)

To prepare cobalt(II) hydroxide and observe its blue-to-pink transformation.

Level: UniversitySafety: Needs supervisionTime: 30 min
Aim of Experiment: To prepare cobalt(II) hydroxide and observe its blue-to-pink transformation.

Theoretical Foundations

Cobalt chloride with NaOH first gives a blue precipitate of basic cobalt salt, which converts to pink Co(OH)2 on standing or warming: CoCl2 + 2NaOH → Co(OH)2↓ + 2NaCl. In air it slowly oxidizes to brown Co(III) species.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 250 mL beaker
  • Glass rod
  • Funnel
  • Filter paper
  • Weighing balance
  • Water bath

Chemical Reagents

  • Cobalt chloride hexahydrate, CoCl2·6H2O (23.79 g)
  • Sodium hydroxide, NaOH (8.0 g)
  • Distilled water (150 mL)

Step-by-Step Practical Procedure

  1. Dissolve 23.79 g CoCl2·6H2O in 80 mL water (pink solution).
  2. Dissolve 8.0 g NaOH in 50 mL water.
  3. Add NaOH with stirring; a blue precipitate forms first.
  4. Warm gently on a water bath; the precipitate turns pink Co(OH)2.
  5. Filter, wash with hot water until free of chloride.
  6. Dry at 110 °C in air-free conditions if possible, and weigh.

Observations & Expected Results

Blue precipitate turning pink; typical yield 8.2–8.9 g of pink powder (surface may brown in air).

Worked Stoichiometric Calculations

Problem: 23.79 g CoCl2·6H2O (M = 237.93) reacts with excess NaOH. Calculate the theoretical yield of Co(OH)2 (M = 92.95). If 8.3 g is obtained, find the percentage yield.

Working: Moles CoCl2·6H2O = 23.79/237.93 = 0.100 mol → 0.100 mol Co(OH)2. Theoretical mass = 0.100 × 92.95 = 9.30 g. Percentage yield = (8.3/9.30) × 100 = 89.2%.

Safety Precautions & Hazard Control

  • Cobalt compounds are toxic; wear gloves.
  • The blue precipitate is a basic salt; warming completes conversion.
  • Protect from prolonged air exposure (oxidizes to brown Co(III)).
  • Wash free of chloride.

Waste Disposal Protocol

Cobalt-containing filtrates go to the heavy-metal inorganic waste container.

Viva Voce Oral Defense Questions & Answers

Q: Why does the precipitate change from blue to pink?

A: The initial blue basic salt converts to pink Co(OH)2 on warming/standing.

Q: What happens to Co(OH)2 in air?

A: It oxidizes to brown cobalt(III) hydroxide species.

Q: Name a use of cobalt compounds.

A: Blue pigments, catalysts, and lithium-ion battery cathodes.

← Back to Experiments Directory