Lead Dioxide from Red Lead and Nitric Acid
To prepare lead dioxide by treating red lead with warm dilute nitric acid.
Theoretical Foundations
Nitric acid dissolves the PbO portion of red lead, leaving PbO2: Pb3O4 + 4HNO3 →(warm) 2Pb(NO3)2 + PbO2↓ + 2H2O. The chocolate-brown PbO2 is filtered, washed, and dried. It is a strong oxidizer used in lead-acid batteries.
Required Apparatus & Chemicals
Laboratory Apparatus
- 250 mL beaker
- Glass rod
- Bunsen burner
- Funnel
- Filter paper
- Weighing balance
- Fume cupboard
Chemical Reagents
- Red lead, Pb3O4 (34.3 g)
- Dilute nitric acid (120 mL)
- Distilled water (for washing)
Step-by-Step Practical Procedure
- Place 34.3 g red lead in a beaker in a fume cupboard.
- Add 120 mL warm dilute nitric acid with stirring.
- Warm gently for 15 minutes; the red powder turns chocolate-brown.
- Filter the brown PbO2; wash with water until the washings are neutral.
- Dry at 110 °C and weigh.
- Test: a little PbO2 with concentrated HCl liberates chlorine.
Observations & Expected Results
Chocolate-brown powder; typical yield 10–11 g; oxidizes HCl to Cl2.
Worked Stoichiometric Calculations
Problem: 34.3 g Pb3O4 (M = 685.60) reacts with excess dilute HNO3. Calculate the theoretical yield of PbO2 (M = 239.20). If 10.5 g is obtained, find the percentage yield.
Working: Moles Pb3O4 = 34.3/685.60 = 0.0500 mol. One mole of Pb3O4 gives one mole of PbO2 = 0.0500 mol. Theoretical mass = 0.0500 × 239.20 = 11.96 g. Percentage yield = (10.5/11.96) × 100 = 87.8%.
Safety Precautions & Hazard Control
- Lead compounds are toxic; wear gloves and a dust mask.
- Work in a fume cupboard; NOx fumes evolve.
- Wash the product free of acid.
- Keep PbO2 away from organic matter (oxidizer).
Waste Disposal Protocol
Lead nitrate filtrate goes to the designated lead waste container.
Viva Voce Oral Defense Questions & Answers
Q: Why does HNO3 leave PbO2 undissolved?
A: PbO2 is insoluble in dilute HNO3; only the PbO portion dissolves as nitrate.
Q: What is the use of PbO2 in batteries?
A: It is the positive plate active material in lead-acid accumulators.
Q: What are the oxidation states of Pb in Pb3O4?
A: Two Pb(II) and one Pb(IV); only Pb(IV) remains as PbO2.