CHEMVEN

Potassium Permanganate from Pyrolusite

To prepare potassium permanganate by fusing pyrolusite (MnO2) with potassium hydroxide and disproportionating the green manganate.

Level: UniversitySafety: Advanced lab onlyTime: 2 h
Aim of Experiment: To prepare potassium permanganate by fusing pyrolusite (MnO2) with potassium hydroxide and disproportionating the green manganate.

Theoretical Foundations

Pyrolusite fused with KOH in air gives green potassium manganate: 2MnO2 + 4KOH + O2 → 2K2MnO4 + 2H2O. Passing CO2 (or adding dilute acid) disproportionates manganate: 3K2MnO4 + 2H2O → 2KMnO4 + MnO2 + 4KOH. The purple permanganate crystallizes on concentration.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Iron crucible
  • Bunsen burner / furnace
  • Glass rod
  • 500 mL beaker
  • Funnel
  • Filter paper
  • China dish
  • Weighing balance

Chemical Reagents

  • Manganese dioxide, MnO2 (17.4 g)
  • Potassium hydroxide pellets, KOH (22.4 g)
  • Potassium nitrate, KNO3 (5 g, oxidant aid)
  • Carbon dioxide source (dry ice or Kipp's)
  • Distilled water (300 mL)

Step-by-Step Practical Procedure

  1. Mix 17.4 g MnO2 intimately with 22.4 g KOH and 5 g KNO3 in an iron crucible.
  2. Fuse the mixture with strong heating, stirring occasionally, until a dark green mass forms.
  3. Cool, extract the green mass with 250 mL warm water, and filter off unreacted MnO2.
  4. Pass CO2 through the green filtrate until it turns deep purple.
  5. Filter off the precipitated brown MnO2.
  6. Evaporate the purple filtrate to the crystallization point and cool.
  7. Filter the dark purple crystals, wash with a little cold water, dry, and weigh.

Observations & Expected Results

Dark purple, almost black, needle-like crystals with metallic lustre; typical yield 14–17 g.

Worked Stoichiometric Calculations

Problem: 17.4 g MnO2 (M = 86.94) is fused as above. Calculate the theoretical yield of KMnO4 (M = 158.0). If 14.5 g is obtained, find the percentage yield.

Working: Moles MnO2 = 17.4/86.94 = 0.200 mol → 0.200 mol K2MnO4. Disproportionation: 3 mol manganate gives 2 mol permanganate, so 0.200 × (2/3) = 0.1333 mol KMnO4. Theoretical mass = 0.1333 × 158.0 = 21.1 g. Percentage yield = (14.5/21.1) × 100 = 68.7%.

Safety Precautions & Hazard Control

  • KMnO4 is a strong oxidizer; keep away from organic matter, glycerol, and concentrated acids.
  • Wear gloves and eye protection during fusion (caustic melt).
  • Do not heat dry KMnO4 above 200 °C (decomposes).
  • Filter through glass wool, not paper, for hot concentrated solutions.

Waste Disposal Protocol

Manganese residues go to the heavy-metal inorganic waste container; never mix permanganate waste with organics.

Viva Voce Oral Defense Questions & Answers

Q: Why does CO2 convert green manganate to purple permanganate?

A: It provides mild acidity that drives the disproportionation 3MnO4(2−) + 2H2O → 2MnO4(−) + MnO2 + 4OH−.

Q: What are the oxidation states of Mn in MnO2, K2MnO4, KMnO4?

A: +4, +6, +7 respectively.

Q: Why is KMnO4 stored in dark bottles?

A: Light catalyzes its decomposition to MnO2, especially in solution.

← Back to Experiments Directory