CHEMVEN

Qualitative Analysis of Solder: Lead and Tin

Dissolve soft solder and confirm Pb and Sn by their classic tests.

Level: UniversitySafety: Advanced lab onlyTime: 60 min
Aim of Experiment: Dissolve soft solder and confirm Pb and Sn by their classic tests.

Theoretical Foundations

Solder (Pb–Sn alloy) dissolves in warm dilute HNO₃: Pb → Pb(NO₃)₂; Sn → metastannic acid (H₂SnO₃, white precipitate) — tin's signature insolubility in HNO₃. Pb²⁺ confirmed by yellow PbCrO₄ or white PbSO₄; tin confirmed by dissolving metastannic acid in HCl and reducing HgCl₂ (white→grey) or the cacotheline violet test.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Beaker
  • Test tubes
  • Fume cupboard
  • Filter paper + funnel

Chemical Reagents

  • Solder pieces
  • Dilute HNO₃ (~4 M)
  • Concentrated HCl
  • K₂CrO₄
  • HgCl₂ (~0.05 M)
  • Cacotheline

Step-by-Step Practical Procedure

  1. Warm solder in dilute HNO₃ (fume cupboard): Pb dissolves; white metastannic acid precipitates.
  2. Filter: filtrate = Pb²⁺; residue = tin as H₂SnO₃.
  3. Filtrate + K₂CrO₄: yellow PbCrO₄ (Pb confirmed).
  4. Dissolve residue in conc. HCl; add to HgCl₂: white→grey (Sn²⁺ confirmed).
  5. Report the alloy components.

Observations & Expected Results

White metastannic acid (Sn); yellow chromate (Pb); HgCl₂ reduction sequence.

Worked Stoichiometric Calculations

Problem: Why does tin give a precipitate with HNO₃ while lead dissolves?

Working: HNO₃ oxidises Sn to insoluble metastannic acid H₂SnO₃; Pb(NO₃)₂ is soluble — a built-in separation.

Safety Precautions & Hazard Control

  • Lead toxicity; NO₂ fumes — fume cupboard.
  • HgCl₂ toxic — gloves.
  • Wear safety goggles and a lab coat throughout the experiment.

Waste Disposal Protocol

Lead/tin/mercury residues segregated to heavy-metal waste.

Viva Voce Oral Defense Questions & Answers

Q: What is metastannic acid?

A: Hydrated tin(IV) oxide, H₂SnO₃ — the white insoluble product of Sn + hot conc. HNO₃.

Q: How is this separation like Group I/II logic?

A: Same principle: exploit a solubility difference (here, nitrate vs oxide) to split two metals.

← Back to Experiments Directory