Flame Test Through Cobalt Glass: Potassium and Sodium Masking

Demonstrate sodium masking of potassium and its removal with cobalt-blue glass.

Level: UniversitySafety: Needs supervisionTime: 25 min
Aim of Experiment: Demonstrate sodium masking of potassium and its removal with cobalt-blue glass.

Theoretical Foundations

Na⁺'s intense 589 nm emission swamps K⁺'s weak lilac lines in mixtures. Cobalt glass absorbs yellow light strongly while transmitting violet — so K⁺'s lilac appears through the glass while Na⁺'s flame looks dark. A single piece of glass turns an impossible observation into a routine one.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Bunsen burner
  • Nichrome wire
  • Cobalt-blue glass pieces
  • Conc. HCl

Chemical Reagents

  • KCl
  • NaCl
  • KCl + NaCl mixture (mostly NaCl)

Step-by-Step Practical Procedure

  1. Flame-test pure KCl: lilac. Pure NaCl: intense yellow.
  2. Flame-test the mixture: yellow dominates, no lilac visible.
  3. View the mixture's flame through cobalt glass: lilac appears.
  4. Increase the Na:K ratio until even the glass struggles — find the limit.

Observations & Expected Results

Mixture: yellow → lilac revealed through blue glass.

Worked Stoichiometric Calculations

Problem: If Na emission is ~100× more intense per mole than K, what Na:K ratio still lets K show through glass? (illustrative)

Working: The glass attenuates Na ~1000×, so roughly up to ~10:1 Na:K remains readable — illustrative only.

Safety Precautions & Hazard Control

  • Burner safety; wire cleaning with conc. HCl — gloves.
  • Wear safety goggles and a lab coat throughout the experiment.
  • Tie back long hair and secure loose clothing before starting.

Waste Disposal Protocol

Salt residues to sink/chemical waste.

Viva Voce Oral Defense Questions & Answers

Q: Does the glass create the lilac colour?

A: No — it only filters; the lilac was always emitted, just overwhelmed.

Q: Why not use the glass for all flame tests?

A: It dims every flame; use it only when sodium masking is suspected.