CHEMVEN

Heating in a Dry Tube: Decomposition Fingerprints

Identify salts by their dry-heating behaviour: gases, sublimates, residues and decrepitation.

Level: UniversitySafety: Needs supervisionTime: 40 min
Aim of Experiment: Identify salts by their dry-heating behaviour: gases, sublimates, residues and decrepitation.

Theoretical Foundations

Dry heating fingerprints: NH₄⁺ salts → NH₃; carbonates → CO₂ (except alkali); nitrates → NO₂/O₂ (brown fumes, except Na/K → nitrite + O₂); hydrated salts → water droplets; Hg²⁺/NH₄⁺ salts may sublime; Zn²⁺ salts → yellow-hot ZnO residue. Litmus at the tube mouth identifies acidic/basic gases.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Dry hard-glass test tubes
  • Bunsen burner
  • Litmus papers
  • Tube holder

Chemical Reagents

  • Ammonium chloride (small)
  • Sodium carbonate (small)
  • Lead(II) nitrate (small)
  • Copper(II) sulphate pentahydrate (small)
  • Zinc carbonate (small)

Step-by-Step Practical Procedure

  1. Heat each dry salt gently, then strongly; observe at each stage.
  2. Test evolved gases with moist litmus at the mouth.
  3. Note sublimates on the cool upper tube, residues' colours hot and cold.
  4. Tabulate the fingerprint for each salt.

Observations & Expected Results

NH₄Cl: white sublimate; Pb(NO₃)₂: brown NO₂, crackling, yellow-hot PbO; CuSO₄·5H₂O: water droplets then black CuO; ZnCO₃: CO₂, yellow-hot ZnO.

Worked Stoichiometric Calculations

Problem: 2Pb(NO₃)₂ → 2PbO + 4NO₂ + O₂. What volume of NO₂ at STP from 3.31 g Pb(NO₃)₂? (illustrative)

Working: 3.31 g = 0.010 mol → 0.020 mol NO₂ = 0.448 L at STP.

Safety Precautions & Hazard Control

  • NO₂ toxic — fume cupboard or tiny amounts.
  • Hot glass looks cool — use holders.
  • Wear safety goggles and a lab coat throughout the experiment.

Waste Disposal Protocol

Residues cooled, then to chemical waste (lead segregated).

Viva Voce Oral Defense Questions & Answers

Q: Why does CuSO₄·5H₂O change colour on heating?

A: Loss of water of crystallisation: blue pentahydrate → white anhydrous → black CuO.

Q: What does a sublimate suggest?

A: NH₄⁺ salts, Hg₂Cl₂/HgCl₂, AlCl₃ — volatile molecular solids.

← Back to Experiments Directory