Diamond versus Graphite: Same Atoms, Opposite Properties

To contrast the physical properties of diamond and graphite and explain them from their bonding and structures.

Level: UniversitySafety: SafeTime: 40 min
Aim of Experiment: To contrast the physical properties of diamond and graphite and explain them from their bonding and structures.

Theoretical Foundations

Both are pure carbon: diamond is a 3D sp³ covalent network (hardness 10, insulator, density 3.51); graphite is sp² sheets with delocalized π electrons and weak interlayer forces (soft, lubricant, conductor along sheets, density 2.26). Structure — not composition — dictates properties: the core lesson of materials science.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Diamond tester or sample (cubic zirconia for comparison)
  • Graphite rods/pencil leads
  • Multimeter
  • Paper
  • Hammer and anvil (optional)

Chemical Reagents

  • Graphite samples
  • Diamond chip or simulant (optional)
  • White paper (for the graphite streak test)

Step-by-Step Practical Procedure

  1. Draw with graphite on paper; try to mark with the diamond — compare hardness.
  2. Measure resistance along a graphite rod (low) versus across a diamond (infinite).
  3. Rub graphite between fingers (lubricity) and note the diamond's rigidity.
  4. Compare densities from handbook values.
  5. Tabulate property versus structure for both.
  6. Discuss which properties come from bonding type.

Observations & Expected Results

Graphite writes, conducts, and feels slippery; diamond scratches everything, insulates, and is rigid — opposite behaviors from identical atoms.

Worked Stoichiometric Calculations

Problem: Diamond density 3.51, graphite 2.26 g cm⁻³ (both pure C). What are their molar volumes, and what does the difference show?

Working: Diamond: 12.011/3.51 = 3.42 cm³ mol⁻¹. Graphite: 12.011/2.26 = 5.31 cm³ mol⁻¹ — graphite's layered structure packs 55% more loosely.

Safety Precautions & Hazard Control

  • No significant hazards.
  • Handle any diamond sample carefully (valuable).
  • Wash hands after graphite (messy).

Waste Disposal Protocol

No waste; samples retained.

Viva Voce Oral Defense Questions & Answers

Q: Why is graphite soft but diamond hard?

A: Weak van der Waals forces between graphite sheets let them slide; diamond is a continuous 3D covalent network.

Q: Why does graphite conduct electricity?

A: Delocalized π electrons move freely within each sp² sheet.

Q: What general lesson does this pair teach?

A: Properties are set by atomic arrangement and bonding, not just elemental composition.