CHEMVEN

Photocatalysis: TiO2 Destroys Dye in Sunlight

To degrade methylene blue with illuminated TiO2 nanoparticles and demonstrate photocatalytic water treatment.

Level: UniversitySafety: Needs supervisionTime: 30 min setup + 2-3 h sunlight
Aim of Experiment: To degrade methylene blue with illuminated TiO2 nanoparticles and demonstrate photocatalytic water treatment.

Theoretical Foundations

UV photons above TiO2's 3.2 eV gap create electron-hole pairs; holes oxidize water to hydroxyl radicals (•OH) that mineralize organic dyes to CO2 and H2O. The dye's blue color vanishes only with both light and TiO2 — the basis of self-cleaning surfaces and solar water purification.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 3 petri dishes
  • Sunlight or UV lamp
  • Stirring rods
  • Color comparison card

Chemical Reagents

  • Methylene blue, dilute (about 150 mL)
  • TiO2 nanopowder (about 0.5 g)
  • White card (color-comparison background)

Step-by-Step Practical Procedure

  1. Put 50 mL dye in each dish: (1) dye only, (2) dye + TiO2 in the dark, (3) dye + TiO2 in sunlight.
  2. Stir dish 3 occasionally.
  3. Photograph all three every 30 minutes.
  4. Compare decolorization after 2-3 hours.
  5. Confirm dish 1 and 2 stay blue while dish 3 fades.
  6. Discuss the need for both catalyst and light.

Observations & Expected Results

Dish 3 bleaches from blue to nearly colorless; dishes 1 and 2 remain blue — proof of true photocatalysis, not adsorption or photolysis alone.

Worked Stoichiometric Calculations

Problem: TiO2 absorbs at λ ≤ 388 nm. What fraction of the solar spectrum's energy is usable (roughly 5% is UV)? What does this imply?

Working: Only about 5% — pure TiO2 uses little sunlight, motivating visible-light photocatalyst research (doping, heterojunctions).

Safety Precautions & Hazard Control

  • UV lamp: goggles; sunlight: avoid heat buildup.
  • TiO2 dust: avoid inhaling.
  • Methylene blue stains; wear gloves.

Waste Disposal Protocol

Filter out TiO2 for reuse; the bleached solution goes down the drain.

Viva Voce Oral Defense Questions & Answers

Q: What are the active species in photocatalysis?

A: Photogenerated holes and the hydroxyl radicals (•OH) they make — powerful oxidizers.

Q: Why are both TiO2 and light needed?

A: Light creates the electron-hole pairs; TiO2 provides the semiconductor bands to separate them.

Q: Name two applications.

A: Self-cleaning glass, solar water disinfection, air purification.

← Back to Experiments Directory