CHEMVEN

Curie Temperature: Nickel Loses Its Magnetism on Heating

To observe nickel losing its ferromagnetism at its Curie temperature (358 °C) and regaining it on cooling.

Level: UniversitySafety: Needs supervisionTime: 45 min
Aim of Experiment: To observe nickel losing its ferromagnetism at its Curie temperature (358 °C) and regaining it on cooling.

Theoretical Foundations

Ferromagnetism comes from aligned atomic magnetic moments; thermal agitation destroys the alignment above the Curie temperature Tc (Ni: 358 °C, Fe: 770 °C, Co: 1121 °C), and the metal becomes paramagnetic. A nickel strip heated in a flame stops being attracted to a magnet near Tc and the attraction returns on cooling — a striking phase transition.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Nickel strip or wire
  • Bunsen burner
  • Strong magnet on a stand
  • Tongs
  • Stopwatch

Chemical Reagents

  • Nickel metal strip (a few grams)
  • Sandpaper (for cleaning oxide)
  • Heat-resistant mat

Step-by-Step Practical Procedure

  1. Suspend the nickel strip near (not touching) the magnet so it is visibly attracted.
  2. Heat the strip in the Bunsen flame with tongs.
  3. Watch the attraction weaken and vanish as Tc is passed.
  4. Remove from the flame and watch the attraction return on cooling.
  5. Estimate the time/temperature region of the transition.
  6. Discuss why the change is reversible.

Observations & Expected Results

The strip visibly pulls away from the magnet when hot (above ~358 °C) and snaps back toward it as it cools — magnetism switching off and on.

Worked Stoichiometric Calculations

Problem: Nickel's Tc is 358 °C. Express it in kelvin.

Working: 358 + 273 = 631 K.

Safety Precautions & Hazard Control

  • Hot nickel causes severe burns; tongs only.
  • Nickel dust/fumes: heat in a ventilated area, do not overheat to melting.
  • Keep the magnet away from the flame.
  • Nickel can cause skin allergy; wash hands.

Waste Disposal Protocol

No waste; the nickel strip is reusable.

Viva Voce Oral Defense Questions & Answers

Q: What is the Curie temperature?

A: The temperature above which a ferromagnetic material becomes paramagnetic as thermal disorder defeats magnetic alignment.

Q: Is the transition reversible?

A: Yes — cooling below Tc restores domain alignment and ferromagnetism.

Q: Why is iron's Tc higher than nickel's?

A: Stronger exchange interaction between Fe moments requires more thermal energy to disorder.