Prussian Blue: An Intense Mixed-Valence Pigment
To synthesize Prussian blue, Fe4[Fe(CN)6]3, and explain its intense color by intervalence charge transfer.
Theoretical Foundations
Mixing Fe³⁺ with [Fe(CN)6]⁴⁻ precipitates Prussian blue: 4Fe³⁺ + 3[Fe(CN)6]⁴⁻ → Fe4[Fe(CN)6]3. Its deep color comes from electron transfer between Fe(II) and Fe(III) across cyanide bridges (intervalence charge transfer), absorbing red-orange light. The open framework also traps Cs⁺, giving medical and environmental uses.
Required Apparatus & Chemicals
Laboratory Apparatus
- 2 beakers
- Stirrer
- Filter funnel and paper
- Test tubes
Chemical Reagents
- Iron(III) chloride FeCl3·6H2O (about 2.7 g)
- Potassium hexacyanoferrate(II) K4[Fe(CN)6]·3H2O (about 4.2 g)
- Distilled water (about 200 mL)
Step-by-Step Practical Procedure
- Dissolve 2.7 g FeCl3·6H2O in 100 mL water (solution A).
- Dissolve 4.2 g K4[Fe(CN)6]·3H2O in 100 mL water (solution B).
- Add B to A slowly with stirring; an intense blue precipitate forms instantly.
- Filter, wash with water, and dry the pigment.
- Test its tinting strength: mix a speck into white paint or chalk.
- Note that the pigment is insoluble and lightfast.
Observations & Expected Results
A deep navy-blue precipitate forms immediately; even a trace tints white base powerfully; the dried pigment is nearly black-blue.
Worked Stoichiometric Calculations
Problem: 2.7 g FeCl3·6H2O (M = 270.30) reacts fully. What mass of Prussian blue (M = 859.23) forms?
Working: Moles Fe³⁺ = 2.7/270.30 = 0.00999 mol. Product = 0.00999/4 = 0.002498 mol. Mass = 0.002498 × 859.23 = 2.15 g.
Safety Precautions & Hazard Control
- Hexacyanoferrates are low hazard but never mix with strong acids (HCN risk).
- FeCl3 stains skin and is corrosive; wear gloves.
- Wash hands after handling.
Waste Disposal Protocol
Collect the filtrate and washings as cyanide-complex waste per local rules; do not acidify.
Viva Voce Oral Defense Questions & Answers
Q: Why is Prussian blue so intensely colored?
A: Intervalence charge transfer: light drives electron hopping between Fe(II) and Fe(III) sites.
Q: Write the formation equation.
A: 4Fe³⁺ + 3[Fe(CN)6]⁴⁻ → Fe4[Fe(CN)6]3.
Q: Name a non-pigment use.
A: Antidote for thallium/cesium poisoning; Cs⁺ removal from nuclear waste.