CHEMVEN

Counting Atoms in Unit Cells: From Corners to Formula Units

To determine Z, the number of atoms or formula units per unit cell, for sc, bcc, fcc, NaCl, CsCl, and diamond by systematic sharing-counts.

Level: UniversitySafety: SafeTime: 40 min
Aim of Experiment: To determine Z, the number of atoms or formula units per unit cell, for sc, bcc, fcc, NaCl, CsCl, and diamond by systematic sharing-counts.

Theoretical Foundations

An atom at a cell corner is shared by 8 cells (counts 1/8), on a face by 2 cells (1/2), on an edge by 4 cells (1/4), and in the body belongs wholly to one cell. Applying these shares gives Z = 1 (sc), 2 (bcc), 4 (fcc and NaCl), 1 (CsCl), and 8 (diamond). Z is the essential input to the density formula.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Unit-cell models or clear diagrams of sc, bcc, fcc, NaCl, CsCl, diamond
  • Worksheet table
  • Colored pens
  • Ruler

Chemical Reagents

  • Printed structure diagrams (sc, bcc, fcc, NaCl, CsCl, diamond)
  • Worksheet table (provided)
  • Highlighter pens (for marking shared atoms)

Step-by-Step Practical Procedure

  1. For the simple cubic cell, count 8 corners × 1/8 and record Z = 1.
  2. For bcc, add the body-center atom: Z = 2.
  3. For fcc, add the 6 face atoms × 1/2: Z = 4.
  4. For NaCl, count Na⁺ (12 edges × 1/4 + 1 body = 4) and Cl⁻ (8 corners × 1/8 + 6 faces × 1/2 = 4): Z = 4.
  5. For CsCl, count corners and body center: Z = 1.
  6. For diamond, add the 4 interior atoms to the fcc 4: Z = 8.
  7. Tabulate Z, coordination number, and APF for all six structures.

Observations & Expected Results

The completed table shows Z = 1, 2, 4, 4, 1, 8 for sc, bcc, fcc, NaCl, CsCl, diamond respectively, with no double counting.

Worked Stoichiometric Calculations

Problem: ZnS (zinc blende) has the diamond-like arrangement with Zn²⁺ on the fcc positions and S²⁻ in half the tetrahedral holes. What is Z?

Working: Fcc Zn²⁺: 4; S²⁻ in 4 of 8 tetrahedral holes: 4. Z = 4 formula units of ZnS per cell.

Safety Precautions & Hazard Control

  • No hazards; modeling exercise only.
  • Take short breaks to avoid eye strain.
  • Store model kits complete after use.

Waste Disposal Protocol

No waste generated.

Viva Voce Oral Defense Questions & Answers

Q: What fraction of an edge atom belongs to one cell?

A: 1/4, because four cells meet at an edge.

Q: In NaCl, how many Na⁺ ions does one unit cell contain?

A: 4: 12 edges × 1/4 = 3 plus 1 at the body center.

Q: Why is Z needed before calculating density?

A: Density needs the mass actually inside one cell: Z × M/NA.

← Back to Experiments Directory