CHEMVEN

Preparation of Soap by Saponification

To prepare soap by alkaline hydrolysis of a vegetable oil and test its properties.

Level: UniversitySafety: Needs supervisionTime: 90 min
Aim of Experiment: To prepare soap by alkaline hydrolysis of a vegetable oil and test its properties.

Theoretical Foundations

Triglyceride + 3 NaOH -> glycerol + 3 soap (sodium carboxylate). Common salt precipitates the soap (salting out); the product is tested for cleansing, pH, and hardness versus a commercial soap.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Beaker (500 mL)
  • Hot plate
  • Glass rod
  • Moulds
  • pH paper
  • Test tubes

Chemical Reagents

  • Coconut or groundnut oil (50 mL)
  • 20% NaOH solution
  • Common salt
  • Distilled water

Step-by-Step Practical Procedure

  1. Warm 50 mL oil to 60 C and add 20% NaOH slowly with vigorous stirring.
  2. Heat with stirring until the mixture thickens and shows no oily drops (saponification complete).
  3. Add saturated salt solution to grain out the soap; let the curd rise.
  4. Scoop the soap curd into moulds and allow to set and cure.
  5. Test pH, lather, and cleansing on an oily cloth versus commercial soap.

Observations & Expected Results

The oil gradually emulsifies into a thick paste; salt separates a firm soap curd that sets into bars with good lather.

Worked Stoichiometric Calculations

Problem: 50 mL of coconut oil (density 0.92 g/mL, SV = 250 mg KOH/g). What mass of NaOH is theoretically needed for complete saponification?

Working: Oil mass = 46 g. KOH needed = 46 x 250/1000 = 11.5 g KOH. NaOH equivalent = 11.5 x 40/56.1 = 8.2 g NaOH theoretical.

Safety Precautions & Hazard Control

  • NaOH solution is caustic; wear gloves and goggles.
  • Stir continuously to prevent spattering of hot caustic paste.
  • Add NaOH slowly to control the exotherm.
  • Cure the soap before skin testing (residual alkali).

Waste Disposal Protocol

Glycerol-salt lye can be neutralised and drained; soap is biodegradable.

Viva Voce Oral Defense Questions & Answers

Q: What is 'graining out'?

A: Adding salt reduces soap solubility (common-ion effect), precipitating the soap curd from the glycerol lye.

Q: Why does soap clean?

A: Its amphipathic molecules form micelles that trap grease inside hydrophobic cores while the hydrophilic exteriors keep them dispersed in water.