CHEMVEN

Cellulose Tests: Schweitzer's Reagent and Iodine-Zinc Chloride

To identify cellulose using its solubility in Schweitzer's reagent and the iodine-zinc chloride stain.

Level: UniversitySafety: Needs supervisionTime: 45 min
Aim of Experiment: To identify cellulose using its solubility in Schweitzer's reagent and the iodine-zinc chloride stain.

Theoretical Foundations

Cellulose dissolves in ammoniacal copper hydroxide (Schweitzer's reagent) and reprecipitates on acidification. With iodine-zinc chloride it stains blue-violet, while lignified fibres stain yellow, distinguishing pure cellulose from wood.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Test tubes
  • Glass rod
  • Microscope slides
  • Dropper
  • Beaker

Chemical Reagents

  • Schweitzer's reagent (ammoniacal Cu(OH)2)
  • Cotton fibres
  • Filter paper
  • Wood shavings
  • Iodine-zinc chloride stain
  • Dilute HCl

Step-by-Step Practical Procedure

  1. Place cotton fibres in 5 mL Schweitzer's reagent and stir; observe dissolution.
  2. Add dilute HCl dropwise to reprecipitate the cellulose as a white mass.
  3. Mount cotton, filter paper and wood shavings on slides with iodine-zinc chloride stain.
  4. Examine colours: blue-violet indicates cellulose, yellow indicates lignin.
  5. Compare cotton (pure cellulose) with wood (lignified).

Observations & Expected Results

Cotton dissolves in Schweitzer's reagent and reprecipitates with acid; iodine-zinc chloride stains cotton and filter paper blue-violet but wood shavings yellow-brown.

Worked Stoichiometric Calculations

Problem: Cellulose is (C6H10O5)n. What is the mass percent of carbon in pure cellulose?

Working: M(unit) = 162; carbon = 6 x 12 = 72. %C = 72/162 x 100 = 44.4%.

Safety Precautions & Hazard Control

  • Schweitzer's reagent releases ammonia; use in a ventilated area.
  • Ammoniacal copper solution stains skin; wear gloves.
  • Add acid slowly to control precipitation.
  • Zinc chloride is corrosive; avoid skin contact.

Waste Disposal Protocol

Neutralise copper-ammonia waste and collect as copper-containing chemical waste.

Viva Voce Oral Defense Questions & Answers

Q: Why does cellulose dissolve in Schweitzer's reagent?

A: The copper-ammonia complex disrupts inter-chain hydrogen bonds of cellulose, solvating the chains.

Q: What does the yellow stain on wood indicate?

A: Lignin, which stains yellow-brown with iodine-zinc chloride, unlike blue-violet cellulose.