Identification of Common Plastics
To identify unknown plastic samples by burn, density and solubility tests.
Theoretical Foundations
Each polymer has signature behaviour: PVC burns with a green flame and HCl fumes, polyethylene drips and smells of paraffin, polystyrene burns with a sooty flame and sweet smell, PET melts and self-extinguishes. Density flotation in water and salt solutions separates polyolefins (float) from PVC/PET (sink), the basis of recycling sorting.
Required Apparatus & Chemicals
Laboratory Apparatus
- Tweezers
- Bunsen burner
- Beakers
- Test tubes
- pH paper
Chemical Reagents
- Unknown plastic chips (PE, PP, PS, PVC, PET)
- Water
- Saturated salt solution
- Toluene
- Litmus/pH paper
Step-by-Step Practical Procedure
- Drop chips in water: note floaters (PE, PP) vs sinkers (PS, PVC, PET).
- Test sinkers in saturated salt solution: PS floats, PVC and PET sink.
- Hold each chip in a flame with tweezers; record flame colour, smoke, smell and dripping.
- Hold moist pH paper in the fumes: HCl from PVC turns it red.
- Confirm with solubility: PS dissolves in toluene, others do not.
- Tabulate results and name each plastic.
Observations & Expected Results
PVC: green flame, choking HCl smell, sinks. PE: blue flame, paraffin smell, floats. PS: sooty orange flame, sweet smell. PET: melts, self-extinguishes.
Worked Stoichiometric Calculations
Problem: A chip sinks in water (density 1.0) but floats in saturated salt solution (density 1.2). Between PS (1.05), PVC (1.4) and PET (1.38), which is it?
Working: Its density is between 1.0 and 1.2, matching polystyrene (1.05). PVC and PET at ~1.4 would sink in the salt solution.
Safety Precautions & Hazard Control
- Burn only tiny chips in a fume cupboard; fumes are toxic.
- Use tweezers; molten plastic burns skin.
- Keep the burner away from solvent bottles.
- Do not inhale fumes directly; waft carefully.
Waste Disposal Protocol
Burnt residues and chips go to solid plastic waste.
Viva Voce Oral Defense Questions & Answers
Q: Why does PVC give a green flame?
A: Chlorine released on heating colours the flame green and forms HCl fumes.
Q: How do recycling plants use density separation?
A: Shredded mixed plastics are floated in water or brine tanks; polyolefins float off while denser plastics sink.