Viscosity of Fuel Oil: Redwood Viscometer
To determine the kinematic viscosity of a fuel oil using the Redwood viscometer.
Theoretical Foundations
Viscosity controls fuel atomisation in burners: too viscous and the spray is coarse, too thin and pumps leak. The Redwood viscometer measures the time for 50 mL of oil to flow through a standard orifice at a fixed temperature (usually 50 or 100 C). The efflux time in seconds converts to kinematic viscosity via the instrument's calibration equation.
Required Apparatus & Chemicals
Laboratory Apparatus
- Redwood viscometer No. 1
- Water bath
- Stopwatch
- 50 mL receiver flask
- Thermometer
Chemical Reagents
- Fuel oil sample (100 mL)
Step-by-Step Practical Procedure
- Clean the viscometer and close the orifice with the ball valve.
- Fill with oil to the mark and bring the bath to 50 C.
- Hold 5 minutes for temperature uniformity.
- Lift the ball and start the stopwatch simultaneously.
- Stop when the receiver reaches 50 mL and record the efflux time.
- Convert seconds to centistokes using the viscometer calibration chart.
Observations & Expected Results
Furnace oil takes 200-400 s at 50 C; light diesel takes under 60 s.
Worked Stoichiometric Calculations
Problem: The efflux time was 180 s, and the calibration gives viscosity = 0.26 x t - 179/t centistokes. Calculate the kinematic viscosity.
Working: Viscosity = 0.26 x 180 - 179/180 = 46.8 - 0.99 = 45.8 cSt at 50 C, typical of a medium fuel oil.
Safety Precautions & Hazard Control
- Maintain the test temperature within 0.5 C.
- Keep the orifice clean; deposits change the flow time.
- Start the watch exactly as the ball lifts.
- Filter the oil to remove particles that could block the jet.
Waste Disposal Protocol
Tested oil goes to the waste-oil container.
Viva Voce Oral Defense Questions & Answers
Q: Why is fuel oil heated before burning?
A: Heating lowers viscosity so the oil atomises into fine droplets that burn completely.
Q: What is the viscosity index?
A: A number showing how little an oil's viscosity changes with temperature; high VI oils are preferred for lubricants.