Total Sulphur in Coal: Eschka Method

To determine total sulphur in coal by the Eschka method.

Level: UniversitySafety: Advanced lab onlyTime: 3 h
Aim of Experiment: To determine total sulphur in coal by the Eschka method.

Theoretical Foundations

Coal is ignited with Eschka mixture (2 parts MgO + 1 part Na2CO3), which oxidises all sulphur (pyritic, sulphate and organic) to soluble sulphate without loss. The sulphate is precipitated as barium sulphate with BaCl2, and the gravimetric factor (S/BaSO4 = 0.1374) gives the sulphur percentage. High sulphur causes SO2 pollution and boiler corrosion.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Muffle furnace
  • Porcelain crucibles
  • Beakers
  • Ashless filter paper
  • Analytical balance

Chemical Reagents

  • Coal sample (1 g)
  • Eschka mixture
  • Hydrochloric acid
  • Barium chloride solution (10%)
  • Distilled water

Step-by-Step Practical Procedure

  1. Mix 1 g coal intimately with 3 g Eschka mixture in a crucible.
  2. Cover with 1 g more Eschka mixture and ignite at 800 C for 1 hour, stirring once.
  3. Digest the cooled mass in hot water, filter, and acidify the filtrate with HCl.
  4. Boil and precipitate with hot BaCl2 solution; digest the precipitate.
  5. Filter through ashless paper, wash free of chloride, ignite and weigh BaSO4.
  6. Calculate S % = BaSO4 weight x 0.1374 x 100 / coal weight.

Observations & Expected Results

Low-sulphur coal gives under 0.1 g BaSO4 per gram; high-sulphur coal gives heavy white precipitates.

Worked Stoichiometric Calculations

Problem: 1.000 g coal gave 0.120 g BaSO4. Calculate the sulphur percentage.

Working: S % = 0.120 x 0.1374 x 100 / 1.000 = 1.65%. A moderately high-sulphur coal needing emission control.

Safety Precautions & Hazard Control

  • Mix coal and Eschka mixture intimately or sulphur is lost as SO2.
  • Do not exceed 800 C; alkali sulphates can decompose.
  • Wash BaSO4 free of chloride or the weight is high.
  • Ignite the precipitate to constant weight.

Waste Disposal Protocol

Barium-containing filtrates go to the heavy-metal waste container.

Viva Voce Oral Defense Questions & Answers

Q: Name the three forms of sulphur in coal.

A: Pyritic (FeS2), sulphate, and organic sulphur bound in the coal structure.

Q: Why does sulphur matter in coal use?

A: It burns to SO2 causing acid rain, and forms sulphuric acid that corrodes boilers and chimneys.