Proximate Analysis: Fixed Carbon by Difference
To calculate fixed carbon from proximate analysis data and grade the coal.
Theoretical Foundations
Fixed carbon is the solid combustible residue after moisture, volatile matter and ash are removed; it is found by difference: FC % = 100 - (moisture + VM + ash). It represents the coke-like carbon that burns with a short hot flame, and higher fixed carbon generally means higher calorific value and higher coal rank.
Required Apparatus & Chemicals
Laboratory Apparatus
- Calculator
- Proximate analysis data sheet
Chemical Reagents
- Results of moisture, volatile matter and ash determinations
Step-by-Step Practical Procedure
- Collect the moisture, VM and ash percentages from the three previous determinations.
- Verify all are on the same basis (as-received or dry).
- Calculate FC % = 100 - (moisture + VM + ash).
- Grade the coal: FC above 70% suggests semi-anthracite; 50-70% bituminous; below 50% sub-bituminous/lignite.
- Estimate calorific value roughly: each 1% FC contributes about 80 kcal/kg.
Observations & Expected Results
A typical bituminous analysis: moisture 3%, VM 28%, ash 18%, FC 51%.
Worked Stoichiometric Calculations
Problem: A coal shows moisture 4.0%, volatile matter 30.0% and ash 16.0%. Calculate fixed carbon and estimate its calorific value.
Working: FC = 100 - (4.0 + 30.0 + 16.0) = 50.0%. Rough CV = 50 x 80 = 4000 kcal/kg (approximate; the bomb calorimeter gives the true value).
Safety Precautions & Hazard Control
- Ensure all three inputs share the same moisture basis.
- Use concordant replicate determinations.
- Remember FC is by difference, so errors in the other three accumulate in it.
- Report the basis clearly (as-received, air-dried or dry).
Waste Disposal Protocol
No additional waste; this is a calculation exercise.
Viva Voce Oral Defense Questions & Answers
Q: Why is fixed carbon not measured directly?
A: Heating coal to drive off volatiles without burning the carbon is impractical; difference is the standard-defined method.
Q: Which rank of coal has the highest fixed carbon?
A: Anthracite, with over 85% fixed carbon and very low volatile matter.