CHEMVEN

Proximate Analysis of Coal: Volatile Matter

To determine the volatile matter of coal (proximate analysis, part 2).

Level: UniversitySafety: Needs supervisionTime: 90 min
Aim of Experiment: To determine the volatile matter of coal (proximate analysis, part 2).

Theoretical Foundations

Volatile matter is the combustible gases (hydrocarbons, CO, H2) driven off when coal is heated at 925 C for 7 minutes excluding air. High VM coals ignite easily and burn with a long flame; low VM coals (anthracite) are hard to ignite. VM also indicates coking potential for metallurgical coal.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Muffle furnace (925 C)
  • Silica crucible with lid
  • Tongs
  • Analytical balance
  • Desiccator

Chemical Reagents

  • Moisture-free coal sample (1 g)

Step-by-Step Practical Procedure

  1. Weigh 1 g of dried coal into the silica crucible and cover with the lid.
  2. Place in the furnace at 925 C for exactly 7 minutes.
  3. Remove, cool in a desiccator, and weigh.
  4. Calculate VM % = loss x 100 / sample weight (on dry basis).

Observations & Expected Results

Bituminous coal gives 20-35% VM with visible flame at the lid; anthracite gives under 10%.

Worked Stoichiometric Calculations

Problem: 1.000 g dry coal weighed 0.720 g after the VM test. Calculate the volatile matter percentage.

Working: VM = (1.000 - 0.720)/1.000 x 100 = 28.0% (dry basis), typical of bituminous coal.

Safety Precautions & Hazard Control

  • Hold exactly 925 C and 7 minutes; the result is method-defined.
  • Keep the lid on to exclude air; burning would inflate the loss.
  • Preheat the furnace before inserting the crucible.
  • Handle the hot crucible only with tongs.

Waste Disposal Protocol

Coked residue goes to solid waste.

Viva Voce Oral Defense Questions & Answers

Q: Why must air be excluded?

A: In air the fixed carbon would burn too, and the loss would no longer measure volatile matter alone.

Q: How does VM affect boiler design?

A: High-VM coals need larger combustion chambers for their long flames; low-VM coals need hotter ignition zones.