To determine the fineness of cement by dry sieving on a 90-micron sieve.

Level: UniversitySafety: SafeTime: 30 min
Aim of Experiment: To determine the fineness of cement by dry sieving on a 90-micron sieve.

Theoretical Foundations

Finer cement hydrates faster and develops early strength sooner because of greater surface area. The standard test sieves 100 g of cement through a 90-micron IS sieve; the residue percentage must not exceed 10% for ordinary Portland cement. Excess coarse residue indicates under-ground clinker and slow strength gain.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 90-micron IS sieve with lid and pan
  • Weighing balance
  • Brush

Chemical Reagents

  • Cement sample (100 g, oven-dried)

Step-by-Step Practical Procedure

  1. Weigh 100 g of dry cement.
  2. Place on the 90-micron sieve, cover, and sieve by gentle shaking for 15 minutes.
  3. Brush the residue lightly without forcing particles through.
  4. Weigh the residue retained on the sieve.
  5. Calculate fineness residue % = residue x 100 / 100.

Observations & Expected Results

Good OPC leaves 5-9% residue; residue above 10% fails the specification.

Worked Stoichiometric Calculations

Problem: 100 g cement left 7.5 g residue on the 90-micron sieve. Does it meet the fineness requirement?

Working: Residue = 7.5%. This is below the 10% maximum, so the cement passes the fineness test.

Safety Precautions & Hazard Control

  • Use oven-dry cement; damp cement agglomerates and will not pass.
  • Sieve gently; aggressive brushing forces coarse particles through.
  • Sieve for the full 15 minutes.
  • Work in a dust mask; cement dust irritates lungs.

Waste Disposal Protocol

Cement residue goes to solid waste, not the drain (it can set in pipes).

Viva Voce Oral Defense Questions & Answers

Q: Why does fineness affect strength?

A: Finer particles expose more surface to water, so hydration and early strength development are faster.

Q: What is the Blaine test?

A: An air-permeability method measuring specific surface area (m2/kg); OPC is typically 225-300 m2/kg.