CHEMVEN

Iodine Value of an Oil by the Wijs Method

To determine the iodine value of an unsaturated oil using Wijs solution.

Level: UniversitySafety: Advanced lab onlyTime: 2 h
Aim of Experiment: To determine the iodine value of an unsaturated oil using Wijs solution.

Theoretical Foundations

The iodine value is the grams of iodine absorbed by 100 g of oil and measures the degree of unsaturation: each double bond adds one molecule of ICl from Wijs solution. Excess ICl is treated with KI to liberate iodine, which is titrated with standard sodium thiosulphate. Drying oils (linseed, about 180) have high values; non-drying oils (coconut, about 10) have low values.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Iodine flasks (glass-stoppered)
  • Burette
  • Pipette
  • Dark cupboard

Chemical Reagents

  • Oil sample (0.2-0.5 g)
  • Wijs solution (ICl in glacial acetic acid, 25 mL)
  • 10% potassium iodide solution
  • 0.1 N sodium thiosulphate (standardised)
  • Starch indicator
  • Carbon tetrachloride or chloroform

Step-by-Step Practical Procedure

  1. Weigh the oil into a dry iodine flask and dissolve in 10 mL carbon tetrachloride.
  2. Add 25 mL Wijs solution, stopper, and keep in the dark for 1 hour (2 hours for highly unsaturated oils).
  3. Add 20 mL KI solution and 100 mL water, then titrate liberated iodine with 0.1 N thiosulphate.
  4. Add starch near the end point and titrate to colourless.
  5. Run a blank identically and calculate IV = (blank - sample) x N x 12.69 / weight of oil.

Observations & Expected Results

The solution changes from deep brown to pale yellow to colourless; linseed oil gives IV 170-190, sunflower 125-140, mustard 100-110.

Worked Stoichiometric Calculations

Problem: 0.30 g oil: blank 42.0 mL, sample 18.5 mL of 0.1 N Na2S2O3. Calculate the iodine value.

Working: IV = (42.0 - 18.5) x 0.1 x 12.69 / 0.30 = 23.5 x 1.269 / 0.30 = 99.4 g I2/100 g. Typical of mustard or rapeseed oil.

Safety Precautions & Hazard Control

  • Keep flasks in complete darkness during the reaction; light causes substitution side-reactions.
  • Use glass-stoppered flasks; iodine monochloride attacks rubber.
  • Add KI solution carefully down the stopper to trap vapours.
  • Standardise thiosulphate on the day of use.

Waste Disposal Protocol

Collect halogenated organic waste in the designated halogenated solvent container.

Viva Voce Oral Defense Questions & Answers

Q: Why is the flask kept in the dark?

A: Light promotes free-radical substitution of iodine into the chain, which would inflate the addition-based iodine value.

Q: What is the difference between drying and non-drying oils?

A: Drying oils have high iodine values and polymerise in air to hard films (used in paints); non-drying oils stay liquid.