Langelier Saturation Index: Corrosivity Assessment
To compute the Langelier Saturation Index (LSI) of a water supply from routine analysis data.
Theoretical Foundations
LSI = pH - pHs, where pHs is the pH at which water is saturated with calcium carbonate, calculated from calcium hardness, alkalinity, TDS and temperature. Positive LSI means scaling tendency; negative LSI means corrosive water. It is a desk calculation using measured pH, Ca hardness, alkalinity, TDS and temperature - no new experiment beyond routine parameters.
Required Apparatus & Chemicals
Laboratory Apparatus
- pH meter
- Thermometer
- Burette set for hardness and alkalinity titrations
- Conductivity meter (for TDS)
- Langelier tables/calculator
Chemical Reagents
- EDTA, buffers, indicators (for Ca hardness)
- Standard H2SO4, indicators (for alkalinity)
- KCl storage solution (electrode)
Step-by-Step Practical Procedure
- Measure pH, temperature, calcium hardness, total alkalinity and TDS of the sample.
- Look up factors A (TDS), B (temperature), C (calcium hardness) and D (alkalinity) from Langelier tables.
- Compute pHs = (9.3 + A + B) - (C + D).
- Calculate LSI = measured pH - pHs.
- Interpret: LSI > 0 scaling; LSI = 0 balanced; LSI < 0 corrosive.
- Recommend treatment (pH adjustment, inhibitors) accordingly.
Observations & Expected Results
Soft acidic upland waters: LSI -1 to -2 (corrosive); hard groundwaters: LSI +0.5 to +1 (scaling).
Worked Stoichiometric Calculations
Problem: Water: pH 7.2, pHs calculated as 7.8. Find LSI and interpret.
Working: LSI = 7.2 - 7.8 = -0.6. Negative, so the water is undersaturated and corrosive to pipes and concrete; pH elevation or corrosion inhibitor dosing is advised.
Safety Precautions & Hazard Control
- Use accurate pH measurement; LSI is sensitive to pH errors.
- Determine calcium (not total) hardness correctly.
- Apply temperature correction for pHs.
- LSI predicts tendency, not rate, of corrosion.
Waste Disposal Protocol
No significant waste; routine titration residues only.
Viva Voce Oral Defense Questions & Answers
Q: What does a positive LSI indicate?
A: The water is supersaturated with CaCO3 and tends to deposit protective (or problematic) scale.
Q: Why is LSI = 0 ideal?
A: The water is in equilibrium with calcium carbonate - neither dissolving protective scale nor depositing excess scale.
Q: Name two ways to correct corrosive water.
A: Raise pH/alkalinity with lime or soda ash; dose a corrosion inhibitor such as polyphosphate.