Chloride Determination: Turbidimetric Silver Chloride Method
To determine chloride in water by turbidimetry of AgCl precipitate at 420 nm.
Theoretical Foundations
Ag⁺ precipitates chloride as colloidal AgCl, whose light scattering is read as apparent absorbance at 420 nm. Nitric acid medium prevents precipitation of Ag2CO3 and Ag3PO4. With uniform precipitation conditions, turbidity is proportional to chloride up to ~10 mg L⁻¹.
Required Apparatus & Chemicals
Laboratory Apparatus
- UV-Vis spectrophotometer
- Volumetric flasks 50 mL
- Pipettes
- Cuvettes
- Brown bottles
Chemical Reagents
- NaCl standard (100 mg L⁻¹ Cl⁻)
- Silver nitrate solution (0.1 M)
- Nitric acid (1 M)
- Unknown water sample
Step-by-Step Practical Procedure
- Pipette 0-5 mL chloride standard into 50 mL flasks (0-10 mg L⁻¹).
- Add 2 mL HNO3 and 2 mL AgNO3 to each; dilute to mark.
- Prepare the unknown identically.
- Wait 10 min in the dark for uniform colloid.
- Zero at 420 nm with the blank; read turbidities.
- Determine chloride from the calibration plot.
Observations & Expected Results
White colloidal turbidity forms; apparent absorbance at 420 nm linear with chloride; typical slope ≈ 0.025 A·L mg⁻¹.
Worked Stoichiometric Calculations
Problem: Slope is 0.025 A·L mg⁻¹ at 420 nm. A sample gives A = 0.375. Find chloride in mg L⁻¹.
Working: c = 0.375/0.025 = 15.0 mg L⁻¹ Cl⁻.
Safety Precautions & Hazard Control
- Keep solutions in the dark; AgCl darkens in light.
- Acidify with HNO3 to stop carbonate/phosphate precipitation.
- Uniform mixing and timing are essential for reproducible colloids.
- Bromide and iodide also precipitate; they are positive interferences.
Waste Disposal Protocol
Collect silver-containing waste in the silver recovery bottle; never mix with chloride waste carelessly.
Viva Voce Oral Defense Questions & Answers
Q: Why is nitric acid added?
A: It keeps the medium acidic so Ag2CO3 and Ag3PO4 cannot precipitate, making the turbidity specific to AgCl.
Q: Why protect AgCl from light?
A: Light photoreduces AgCl to dark metallic silver, changing particle size and colour and ruining the turbidity reading.
Q: Why is this turbidimetry, not colorimetry?
A: AgCl is white; the signal comes from scattered light, not from absorption of a coloured species.