Magnesium in Talc

Determine magnesium in commercial talc powder by pyrophosphate gravimetry.

Level: UniversitySafety: Needs supervisionTime: 4 h
Aim of Experiment: Determine magnesium in commercial talc powder by pyrophosphate gravimetry.

Theoretical Foundations

Talc, Mg3Si4O10(OH)2, is decomposed by fusion or strong acid digestion; silica is filtered off and magnesium precipitated as MgNH4PO4, ignited to Mg2P2O7 (GF = 0.2184). Commercial talc is often diluted with carbonates or chlorite, so the found % Mg indicates the talc content versus pure mineral (19.22% Mg).

Required Apparatus & Chemicals

Laboratory Apparatus

  • Analytical balance
  • Platinum or nickel crucible
  • Muffle furnace
  • 400 mL beaker
  • Ashless filter paper
  • Porcelain crucible
  • Desiccator

Chemical Reagents

  • Talc powder sample
  • Sodium carbonate (for fusion)
  • Hydrochloric acid, dilute
  • Diammonium hydrogen phosphate solution, 10%
  • Ammonia solution
  • Distilled water

Step-by-Step Practical Procedure

  1. Weigh accurately 0.5 g talc; fuse with 3 g Na2CO3 at 1000 C for 20 minutes.
  2. Dissolve the melt in dilute HCl; evaporate to dehydrate silica and filter it off.
  3. Dilute the filtrate to 150 mL; add 15 mL 10% (NH4)2HPO4.
  4. Precipitate with concentrated ammonia as usual; stand 4 hours.
  5. Filter, wash with dilute ammonia, ignite at 1000 C to constant mass.
  6. Weigh Mg2P2O7; calculate % Mg.

Observations & Expected Results

Fusion gives a clear melt; silica filtered off; white Mg2P2O7, typically about 0.16 g from 0.5 g commercial talc.

Worked Stoichiometric Calculations

Problem: 0.5000 g of talc gave 0.1580 g Mg2P2O7. Calculate % Mg. (Pure talc = 19.22% Mg)

Working: Mass Mg = 0.1580 × 0.2184 = 0.03451 g. % Mg = (0.03451/0.5000) × 100 = 6.90% — well below 19.22%, showing this commercial powder is heavily diluted with non-talc minerals.

Safety Precautions & Hazard Control

  • Fuse completely; unfused talc gives low results.
  • Remove silica fully before the phosphate precipitation.
  • Use a platinum or nickel crucible for the carbonate fusion.

Waste Disposal Protocol

Alkaline fusion residues neutralised; filtrates to aqueous waste.

Viva Voce Oral Defense Questions & Answers

Q: Why fuse talc instead of dissolving it in acid?

A: Talc's silicate lattice resists acid attack; carbonate fusion breaks it down into soluble silicate and free MgO.

Q: What does the low % Mg tell you?

A: The sample is not pure talc — it contains diluents such as carbonates, quartz or chlorite that contribute mass but little magnesium.