CHEMVEN

Magnesium in Dolomite as Magnesium Pyrophosphate

Determine magnesium in dolomite after removing calcium as oxalate, weighing as Mg2P2O7.

Level: UniversitySafety: Needs supervisionTime: 4 h
Aim of Experiment: Determine magnesium in dolomite after removing calcium as oxalate, weighing as Mg2P2O7.

Theoretical Foundations

This is the second half of the classical dolomite analysis (see experiment 055). After calcium oxalate is filtered off, the filtrate contains magnesium, which is precipitated as magnesium ammonium phosphate: Mg2+ + NH4+ + HPO4 2- → MgNH4PO4(s) + H+. Ignition converts it: 2MgNH4PO4 → Mg2P2O7 + 2NH3 + H2O. The gravimetric factor for magnesium is 2 × M_Mg/M_Mg2P2O7 = 48.61/222.56 = 0.2184.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Analytical balance
  • 400 mL beaker
  • Hot plate
  • Ashless filter paper
  • Porcelain crucible
  • Muffle furnace at 1000 C
  • Desiccator

Chemical Reagents

  • Dolomite sample
  • Hydrochloric acid, dilute
  • Ammonium oxalate solution, 4%
  • Diammonium hydrogen phosphate solution, 10%
  • Ammonia solution, concentrated and dilute
  • Distilled water

Step-by-Step Practical Procedure

  1. Dissolve 0.5 g dolomite in dilute HCl; remove calcium as oxalate at pH ~5 and filter it off (experiment 055).
  2. Acidify the combined filtrate with HCl and concentrate to 150 mL.
  3. Add 15 mL 10% (NH4)2HPO4 solution.
  4. Add concentrated ammonia dropwise with vigorous stirring until strongly alkaline, then 10 mL excess.
  5. Let stand 4 hours (or overnight) for complete crystallisation.
  6. Filter through ashless paper; wash with dilute ammonia (1+20).
  7. Ignite at 1000 C to constant mass; cool and weigh Mg2P2O7.
  8. Calculate % Mg.

Observations & Expected Results

White crystalline MgNH4PO4 forms slowly; ignited residue is white Mg2P2O7, typically about 0.30 g from 0.5 g dolomite.

Worked Stoichiometric Calculations

Problem: 0.5000 g of dolomite gave 0.2980 g Mg2P2O7. Calculate % Mg. (GF_Mg = 0.2184; theoretical Mg in dolomite = 13.18%)

Working: Mass Mg = 0.2980 × 0.2184 = 0.06508 g. % Mg = (0.06508/0.5000) × 100 = 13.02% (98.8% of the theoretical 13.18%).

Safety Precautions & Hazard Control

  • Remove calcium first; Ca2+ would precipitate as Ca3(PO4)2.
  • Add ammonia slowly with stirring or the precipitate is slimy.
  • Wash with dilute ammonia, not water, to prevent peptization.
  • Ignite at 1000 C to expel all ammonia and water.

Waste Disposal Protocol

Ammoniacal phosphate filtrates to aqueous waste.

Viva Voce Oral Defense Questions & Answers

Q: Write the ignition reaction of magnesium ammonium phosphate.

A: 2MgNH4PO4 → Mg2P2O7 + 2NH3↑ + H2O↑.

Q: Why wash with dilute ammonia?

A: MgNH4PO4 is appreciably soluble in pure water; dilute ammonia suppresses its solubility by the common-ion effect and prevents peptization.

Q: Why let the precipitate stand for hours?

A: MgNH4PO4 crystallises slowly; standing ensures complete precipitation and large, pure, filterable crystals.