Purity of Gypsum: Sulfate as BaSO4

Determine the purity of a gypsum sample (CaSO4·2H2O) via its sulfate content.

Level: UniversitySafety: Needs supervisionTime: 2 h
Aim of Experiment: Determine the purity of a gypsum sample (CaSO4·2H2O) via its sulfate content.

Theoretical Foundations

Gypsum dissolves in hot dilute HCl, releasing sulfate: CaSO4·2H2O → Ca2+ + SO4 2- + 2H2O. Precipitation with BaCl2 gives BaSO4 (Ksp = 1.1 × 10^-10), which is far less soluble than CaSO4, so precipitation is quantitative. Comparing the found % SO4 with the theoretical 55.79% for pure CaSO4·2H2O (96.06/172.17) gives the purity.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Analytical balance
  • 400 mL beaker
  • Hot plate
  • Ashless filter paper
  • Muffle furnace
  • Desiccator

Chemical Reagents

  • Gypsum sample, ground
  • Hydrochloric acid, dilute
  • Barium chloride solution, 10% w/v
  • Silver nitrate solution, 0.1 M
  • Distilled water

Step-by-Step Practical Procedure

  1. Weigh accurately 0.5-0.6 g of ground gypsum.
  2. Dissolve in 200 mL hot water containing 5 mL dilute HCl with stirring.
  3. Heat to near boiling; precipitate with 10 mL hot 10% BaCl2 dropwise.
  4. Digest 1 hour, test supernatant, filter and wash chloride-free.
  5. Ignite at 800 C to constant mass; cool in desiccator and weigh BaSO4.
  6. Calculate % SO4 and hence % purity of CaSO4·2H2O.

Observations & Expected Results

Gypsum dissolves slowly in hot acid; white BaSO4 precipitates. Typical ignited mass about 0.80 g from 0.6 g sample.

Worked Stoichiometric Calculations

Problem: 0.6000 g of gypsum gave 0.7970 g BaSO4. Calculate % SO4 and the purity of the gypsum. (Theoretical SO4 in CaSO4·2H2O = 55.79%)

Working: Mass SO4 = 0.7970 × 0.4116 = 0.3280 g. % SO4 = (0.3280/0.6000) × 100 = 54.67%. Purity = (54.67/55.79) × 100 = 98.0% CaSO4·2H2O.

Safety Precautions & Hazard Control

  • Grind the gypsum finely so it dissolves completely.
  • Keep the solution hot during dissolution; gypsum is only sparingly soluble cold.
  • Do not confuse surface moisture with purity loss; dry the sample at 40 C if damp.

Waste Disposal Protocol

Barium filtrates to heavy-metal waste.

Viva Voce Oral Defense Questions & Answers

Q: Why does BaSO4 precipitate quantitatively even though CaSO4 was already present?

A: BaSO4 (Ksp ≈ 1.1 × 10^-10) is about 10^5 times less soluble than CaSO4, so adding Ba2+ drives sulfate essentially completely into BaSO4.

Q: What impurities lower the apparent purity of gypsum?

A: Clay, silica, calcium carbonate and surface moisture — carbonate is removed as CO2 by the acid.

← Back to Experiments Directory