Column Chromatography: Purifying Copper Sulfate from Nickel Impurity

To separate Cu2+ from Ni2+ on an alumina/cellulose column by selective elution and determine the recovery of copper.

Level: UniversitySafety: SafeTime: 2 h
Aim of Experiment: To separate Cu2+ from Ni2+ on an alumina/cellulose column by selective elution and determine the recovery of copper.

Theoretical Foundations

On an alumina column, Ni2+ forms a more strongly retained band than Cu2+ under mildly acidic elution, or the order is tuned with HCl concentration via chloro-complex formation. Eluting with dilute HCl washes Ni2+ through at a different rate than Cu2+, giving two coloured bands (blue Cu, green Ni). Fractions are analysed spectrophotometrically or by titration; recovery = Cu recovered / Cu loaded.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Glass column
  • Alumina or cellulose powder
  • Fraction tubes
  • Spectrophotometer

Chemical Reagents

  • CuSO4 + NiSO4 mixture (known Cu content)
  • Dilute HCl eluents (0.5 M, 2 M)
  • Distilled water

Step-by-Step Practical Procedure

  1. Pack the column as an aqueous slurry.
  2. Load the Cu/Ni mixture as a narrow band.
  3. Elute with 0.5 M HCl, collecting 5 mL fractions.
  4. Note the coloured bands and pool Cu-containing fractions.
  5. Increase to 2 M HCl to strip Ni2+.
  6. Determine copper in the pooled fractions (iodometric titration or A810).
  7. Calculate % recovery of copper and check Ni contamination.

Observations & Expected Results

Blue copper band elutes separately from the green nickel band; recoveries of 90-98% Cu with <2% Ni are typical.

Worked Stoichiometric Calculations

Problem: Loaded 0.500 g Cu; recovered 0.472 g. What is the % recovery?

Working: Recovery = 0.472/0.500 x 100 = 94.4%.

Safety Precautions & Hazard Control

  • Do not let the bed run dry.
  • Handle HCl in a ventilated area.
  • Load as a narrow band for clean separation.

Waste Disposal Protocol

Metal-containing fractions to heavy-metal aqueous waste; packing to solid waste.

Viva Voce Oral Defense Questions & Answers

Q: On what basis do Cu2+ and Ni2+ separate here?

A: Different adsorption affinities for the stationary phase (and different chloro-complex stabilities), giving different migration rates under the HCl gradient.

Q: How would you detect Ni contamination in the Cu pool?

A: Dimethylglyoxime test (red Ni complex) or visible spectrophotometry at Ni's absorption maximum.